Hello,
Been awhile since I've been on this forum. I have a 250ex that I bought new in 2012. I've noticed the arc starting getting harder and harder and now I have to touch the work piece to get things going. Welds fine after that. My set up is water cooler, scc pedal and flex loc head.
Things I checked...
1) my torch is plugged in the negative
2) I cleaned my ground clamp.
3) I cleaned my work piece and tried a new tungsten
4) went back to original pedal and torch
5) tried using thumb switch.
6) removed cover and set gap to 0.30 it was over 0.40
7) I see no spark across the gap when trying to weld looking threw front cover.
8) turned preflow down and waited 8 seconds with foot pedal pressed, no arc
Anything else I can try before call tech support?
Thanks for any help