  1. Default What is arc Force?

    I was looking at the EX250 as opposed to the LX225 I bought the latter, (I love the machine by the way). I still can't find any explaination of what Arc Force is, The welding tips and tricks guy blew it off saying it had something to do with stick welding. I've looked in all the welding books I have and can find no reference to arc force. It's not really important but it's been nagging at me. Anybody got an explaination?

  2. #2

    Default

    pmill,

    The arc force control is also known as dig. It affects the stick welding qualities, especially when the rod is pushed it close, it automatically compensates for the drop in voltage by boosting the amps. It also can determine how well a weld puddle wets into the side, or in other words, how fluid the puddle is and how soft the arc can be.

    The inductance is related to mig. It can be called pinch effect, inductance, dig, arc force etc. In mig, the arc force responds to wire burn off rate and affects amp rise timing between burnoff.

  3. #3
    Join Date
    Jul 2010
    Location
    Port Saint Lucie , Florida
    Posts
    85

    Default

    Yeah what Mark said..

    I still havent used the stick function on mine yet.
    Havent needed to..

Similar Threads

  1. 250ex Arc Force not working?
    By Monty in forum Stick Welding (SMAW)
    Replies: 2
    Last Post: 08-21-2016, 01:58 AM
  2. Arc Force Question
    By plumber in forum Stick Welding (SMAW)
    Replies: 30
    Last Post: 01-23-2013, 03:05 PM
  3. 6010 Arc Force settings
    By betokasu in forum Stick Welding (SMAW)
    Replies: 3
    Last Post: 04-28-2012, 04:02 AM
  4. Arc Force
    By Buzz in forum TIG Welding (GTAW/GTAW-P)
    Replies: 7
    Last Post: 01-19-2012, 06:24 AM
  5. arc force control for powertig 200lx
    By britstef in forum TIG Welding (GTAW/GTAW-P)
    Replies: 1
    Last Post: 03-30-2010, 02:34 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •