Originally Posted by
christian
I could be mistaken, but I recall on the Weld.com forum somewhere, that an upgraded Nova foot pedal being passed along to Bob Moffat after this video.
Kevin Caron, in his video demo of the unit seemed to have no trace of a sputter with the OEM pedal, if that's what he was using.
I upgraded to an SSC pedal for my 210EXT shortly after getting my unit, a few years ago. Now Everlast has the Nova upgrade foot pedal, rather than an SSC branded one, but they are both undoubtedly better than the OEM pedal.
Or, maybe it's your torch/tungsten.
Post a pic of your torch, with the tungsten newly prepped and at your usual stick-out for us to see, in case there's something at that end.
Otherwise, call Everlast if there's nothing for us to spot.
And please do let us all know if you do get an upgraded pedal, and if you find that it improves things.