    Greetings,

    My itig200T is coming on 6th month and I've been generally happy with the performance.

    There is, however, a strange behavior I am seeing. When tapering off with the pedal at the end of weld, sometimes I get a spike of current towards the end, when I am easing up on the pedal. Say, I am getting down to 40A, then all of a sudden I get a full blast at 125A right before the arc extinguishes. Haven't had a way to look at the panel when this happens, so it is just my judgment of what is happening.

    It is very annoying when that happens near the edge, because it pretty much guarantees a nice blow-through. It does not happen all the time, maybe twice every 5 welds.

    To me, behavior is very similar to what would happen with dirty (scratchy) pot. So I looked inside the pedal.

    The pedal (has FT-47K-CL on the back) has small caps soldered across pot pins to deal with scratchiness, I presume. I was surprised to see that the insides of the pedal are squeaky clean. Visually the pot does not appear to be of cheap variety and seems well sealed. The pedal is very well constructed. So no I am not really sure.

    Settings: no pulse, peak at 125A, start 20A end 20A, 0s up/down slope, 2T, 0.5s pre flow, 10s post flow.

    Looking for ideas on how to pinpoint the cause and/or avoid the issue. All suggestions much appreciated.

    -rC

  2. Default

    Gee,

    It seems like you've touched all of the proverbial bases. I mean, it sounded like your end amp setting might have been higher than the minimum, which would cause as much, undoubtedly.

    Since those items apparently have a 6 month warranty, I'd send it in to Everlast for a repair or replacement. Give them a call for an RMA number.

    Or I might just buy one of their new upgraded NOVA pedals. I mean, I bought an upgraded SSC pedal for my 2015 210EXT right after getting the welder, as it seemed a sensible upgrade, much like I also immediately upgraded to a Superflex torch hose/cable.
    Everlast 210 EXT (2015)

    www.youtube.com/newjerusalemtimes

  3. #3
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by rcross View Post
    Looking for ideas on how to pinpoint the cause and/or avoid the issue. All suggestions much appreciated.
    I think you called it, sounds like a bad spot in the pot to me, too. One way to pinpoint would be to test the pot with a meter that has a min max function or a DSO. Or just replace the pot and see if the problem is gone.
    For a way to avoid the issue, set the machine to use the downslope function then you don't need to do a manual tapering off. (not a real fix, but you did ask how to avoid)
    Long arc, short arc, heliarc and in-the-dark!

  4. Default

    Yes, I tried the multimeter, even LCR meter, but those digital ones usually have a slow analog to digital converter, so it is rather hard to catch transient events with it. I really need to hook the DSO up.

    For the downslope to work, I would need to just get off the pedal abruptly and then let the downslope to run its course, right?

    Thank you for the suggestion.

  5. #5

    Default

    Just a cheap 10.00 needle meter would work better, more than likely.
    Make sure you test both sides. Something is causing it to surge. Could be the machine, but most issues are in the pedal.

  6. Default

    Thank you for the suggestion. I will try the analog multimeter too.

    Do you happen to know the voltage that is applied across the pot when the pedal is connected to the machine? I assume it is quite a bit higher than my multimeter is putting out.

  7. #7

    Default

    I don't know the voltage off hand but it won't matter when you test the pins according to the plug pinout in the manual. I don't think it is higher than a few volts anyway.

Similar Threads

  1. Replies: 27
    Last Post: 08-21-2012, 04:47 PM
  2. Strange
    By Rambozo in forum Welding Repairs
    Replies: 6
    Last Post: 07-12-2012, 02:44 AM

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •