Share
Results 1 to 7 of 7

Thread: Chrome Vanadium handtools

  1. Default Chrome Vanadium handtools

    I need to make a stubby combination wrench cutting the middle from one and joining the two ends. The wrench was picked up at a garage sale has chrome vanadium stamped on it.

    What rod do I use and are there any tips or tricks for welding this metal?

    Appreciate any pointers.

  2. #2
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    What welding process are you going to use?
    Long arc, short arc, heliarc and in-the-dark!

  3. #3
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Didn't notice this was in the TIG category. I would say ER70 or ER80 would do the job. Vee out the joint and try to limit the heat input and you should end up with something close to the original strength. Since you are going shorter, I'm sure it will be plenty strong.
    Long arc, short arc, heliarc and in-the-dark!

  4. Default

    I have some ER70 on hand. I think I'll cut the waste in half and see how it works before I join the ends. Thanks!

  5. #5

    Default

    Grind the chrome back a little and it welds easy.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  6. Default

    Sounds good, will do. Thanks!

  7. Default

    This might be too late but I just saw this post.

    http://www.lincolnelectric.com/en-us...s-312-rod.aspx