A lot of Harbor Freight metal working tools need improving right out of the box to make them precise and accurate implements. I consider the effort much like building a Heathkit electronic device from years back.

Funny thing... One gets to the point in their DIY career where they spend more time building and modifying tools rather than using them.

The goal of this effort is to configure the press ram with gibs to bring a horrible amount of slop down to zero.

Today's effort was just idea sorting out and template creation with cardboard standing in for metal and the hot glue gun substituting for the welder.

The bracket will eventually sport stubby bolts pushing gib plates against the press frame removing the ram slop.