    Default Wp-20 hose routing

    Received an Everlast cooler yesterday and I searched for a thread I thought I saw about the Everlast torch water hose colors being backwards.
    Didn't find the thread but to route them in the right direction doesn't that put the blue hose in the red connector and the red hose
    in the blue?? Just checking, Thanks

  2. #2

    Default

    The best way to determine which goes where is to blow through the hoses and listen to the torch. If you blow through and hear air hissing out the torch, that's your gas line. If you blow through another hose and the air exits out the remaining hose, it's a water line. The water hoses should be routed so that water exits the hose that also acts as the power cable. The water feed is the other hose. The power/water hose fitting should also be left hand threaded but just the basics I just explained should help you out.
    Everlast 250EX with cooler and WP20 Torch
    Millermatic Mig Welder
    Gas welding setup
    A bunch of Snap-On tools
    And a Brain

  3. #3
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by azsprint6 View Post
    Received an Everlast cooler yesterday and I searched for a thread I thought I saw about the Everlast torch water hose colors being backwards.
    Didn't find the thread but to route them in the right direction doesn't that put the blue hose in the red connector and the red hose
    in the blue?? Just checking, Thanks
    Nope, the hose colors should be getting better but you need to check your actual torch to make sure. Quite a few people have hooked it up wrong because it is somewhat non intuitive if you are new to this. The best way to figure out the hoses is to blow in them one at a time. On one you will feel air coming out of the end of the torch (cup), that is your argon line. The hose coming out of the power plug is the water return line and goes in the red or IN port on your cooler. The last hose you have left is the water supply and that goes to the blue or OUT on the cooler. If the colors are right, that's great, but you never know. This way you will always get it right first time, and not get your argon hose all contaminated with coolant.
    Long arc, short arc, heliarc and in-the-dark!

  4. #4
    Join Date
    Oct 2013
    Location
    Glendale Arizona
    Posts
    26

    Default

    Thanks for the replies. The Everlast Wp-20 hose connected to the dinse connector is blue, the red one is the long one going to the torch head. Black long one is gas.
    I'm actually replacing a Longevity 110v to the Everlast 220v so I can plug it to the back of the 255. The water hoses on the torch I was using were both black, gas hose blue. I had the short dinse connector hose going to the inlet on the cooler.

Similar Threads

  1. Moving to a Standard Ar/Co2 Hose
    By minitruckn' in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 2
    Last Post: 10-25-2014, 11:24 AM
  2. Got a new torch with Superflex hose-WOW!!
    By Scetoaux in forum TIG Welding (GTAW/GTAW-P)
    Replies: 30
    Last Post: 09-10-2013, 09:52 PM
  3. Polished Air Hose Holder, Too Simple
    By cbmkr in forum Other Custom Fabrications
    Replies: 0
    Last Post: 08-20-2012, 08:18 PM
  4. Radnor Welding Hose 1/4" x 50' Twin Torch Hose
    By cbmkr in forum Buy, Sale or Trade
    Replies: 0
    Last Post: 08-17-2012, 03:40 PM
  5. Hose included with PP205
    By rengaw21001 in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 1
    Last Post: 02-27-2011, 06:25 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •