    Quote Originally Posted by 2horses View Post
    Well, I got to try my torch today. I must have overheated it because it's leaking. Can i just replace the torch or do i have to buy all new hoses?
    Usually it's not the torch, but the power line that fails first. If you're lucky you can just replace that. However, if it got real hot, it might have melted holes in the other two lines. All the parts are available separately, so you can replace what you need.

    BTW: CK makes a fuse block connector that will save your torch and lines if you lose water flow for any reason.
    Last edited by Rambozo; 03-08-2017 at 11:50 PM.
    Long arc, short arc, heliarc and in-the-dark!

  2. Default

    Thanks,I'll have to investigate to see where the coolant is leaking.
    I am going to buy a CK Flexloc torch, but would like to fix this one.
    I'll look into that fuse block.

  3. #3
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Long arc, short arc, heliarc and in-the-dark!

  4. #4

    Default

    Your lines may be connected wrong if you have coolant coming out where the gas should.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  5. Default

    Thanks for the video.
    Definitely going to buy one of them Fuse Blocks.
    I don't know what caused my cooler to air lock, but don't want to loose another power cable if it ever happens again.

Similar Threads

  1. Using water cooled torch as air cooled?
    By Fusion in forum TIG Welding (GTAW/GTAW-P)
    Replies: 16
    Last Post: 01-16-2014, 10:08 AM
  2. WP-18 15' Water Cooled Tig Torch Available and What Style
    By cbmkr in forum TIG Welding (GTAW/GTAW-P)
    Replies: 6
    Last Post: 12-20-2012, 05:07 PM
  3. Change tig torch to a smaller water cooled torch
    By wheelrdealer in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 4
    Last Post: 09-18-2012, 04:07 PM
  4. water cooled torch
    By D.C. Metal Designs in forum General Welder Questions
    Replies: 7
    Last Post: 08-11-2010, 04:01 AM
  5. Water cooled torch and cooler
    By WAYNESWORLD in forum TIG Welding (GTAW/GTAW-P)
    Replies: 9
    Last Post: 09-11-2009, 04:33 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •