Share
Results 1 to 11 of 11

Thread: Water cooled torch getting hot?

  1. Default Water cooled torch getting hot?

    I recently bought a 255 EXT..Works Great.
    The only problem i'm having is that the torch is getting really hot?
    Last night i was welding for about a half hour ( not continuous,couple minute breaks between welds))at 125 amps and my water cooled torch that comes with the machine was getting really hot.
    I checked the cooler and it was pumping just fine.
    checked to make sure the lines weren't kinked
    I hate to see what it does at higher amps.
    Is anyone else having this problem, or is there something restricting the flow through the torch?

  2. #2

    Default

    Slide the torch handle back to see if a line is kinked or damaged. You could also turn the pump on for a second with the return line disconnected to be sure you have flow.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  3. Default

    Yea, something's wrong... I'll weld for 1/2hr @250A and never feel any real heat in the torch (other than the cup). I can make 3 - 4 tungsten changes without concern for it. Mine is an old Miller cooler with a clear flow indicator on the return so flow's really evident. When I went from the torch that came with my 256 to a CK I was worried that the flow was so much less than it was but, after talking to them, I measured what came out of the return line into a lg soda cup (I forget the oz/min but it wasn't as much as I thought it would be). Do that for yours and see what you get as zoama suggested.

  4. Default

    Thanks for the help
    I went out this morning and took the cover off the cooler and could see that the coolant wasn't circulating through the lines.
    the pump was air locked, so i pulled the little blue line out of the tank and sucked through it while it was running and primed the pump. it's working good now.
    Yeah i got a mouth full of coolant...
    i know now to take the cap off and make sure it's pumping before welding...I should have known better

  5. Default

    Well, I got to try my torch today. I must have overheated it because it's leaking. Can i just replace the torch or do i have to buy all new hoses?

  6. #6
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by 2horses View Post
    Well, I got to try my torch today. I must have overheated it because it's leaking. Can i just replace the torch or do i have to buy all new hoses?
    Usually it's not the torch, but the power line that fails first. If you're lucky you can just replace that. However, if it got real hot, it might have melted holes in the other two lines. All the parts are available separately, so you can replace what you need.

    BTW: CK makes a fuse block connector that will save your torch and lines if you lose water flow for any reason.
    Last edited by Rambozo; 03-08-2017 at 11:50 PM.
    Long arc, short arc, heliarc and in-the-dark!

  7. Default

    Thanks,I'll have to investigate to see where the coolant is leaking.
    I am going to buy a CK Flexloc torch, but would like to fix this one.
    I'll look into that fuse block.

  8. #8
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Long arc, short arc, heliarc and in-the-dark!

  9. #9

    Default

    Your lines may be connected wrong if you have coolant coming out where the gas should.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  10. Default

    Thanks for the video.
    Definitely going to buy one of them Fuse Blocks.
    I don't know what caused my cooler to air lock, but don't want to loose another power cable if it ever happens again.

  11. #11

    Default

    was it vapor locked day one or did it happen later? And another tip is fill coolant with torch and line on ground or lower than cooler, that way all the air rises as it fills. I do this and even top it off while running just to make sure its all full of coolant.

    Barry

Similar Threads

  1. Using water cooled torch as air cooled?
    By Fusion in forum TIG Welding (GTAW/GTAW-P)
    Replies: 16
    Last Post: 01-16-2014, 10:08 AM
  2. WP-18 15' Water Cooled Tig Torch Available and What Style
    By cbmkr in forum TIG Welding (GTAW/GTAW-P)
    Replies: 6
    Last Post: 12-20-2012, 05:07 PM
  3. Change tig torch to a smaller water cooled torch
    By wheelrdealer in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 4
    Last Post: 09-18-2012, 04:07 PM
  4. water cooled torch
    By D.C. Metal Designs in forum General Welder Questions
    Replies: 7
    Last Post: 08-11-2010, 04:01 AM
  5. Water cooled torch and cooler
    By WAYNESWORLD in forum TIG Welding (GTAW/GTAW-P)
    Replies: 9
    Last Post: 09-11-2009, 04:33 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •