Thread: Mig 210 Spool gun problem fixed; READ

  1. Default Mig 210 Spool gun problem fixed; READ

    I was having all kinds of erratic burn back and bead issues welding 1/4” AL. After checking everything, I took the gun apart and found the problem. The drive gear on the feeder motor was not tight and let the wire slip and even stop feeding altogether, at times. As you can imagine having a very inconsistent wire speed makes it impossible to get a decent weld. I cleaned off the shaft and put the gear back with some green (wick n loc) loctite. Now welding AL is almost too easy.
    FWIW, when looking for the problem, I held the feeder wheel and it would actually stop if I held too hard. Then is when I thought it was either a bad motor or something was slipping.
    Hope this helps if you're not happy with welding AL. It may be the gun and not you.
    Pete
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	gear.jpg 
Views:	556 
Size:	112.8 KB 
ID:	13550  

Similar Threads

  1. Helmet Shootout: W60 Truesight vs Harbor Freight Blue Flame vs HSL-100 fixed shade
    By jakeru in forum Tips & Tricks, Custom Tools, Safety, Ideas and Reviews.
    Replies: 43
    Last Post: 11-19-2012, 07:42 PM
  2. pedal issue is fixed!!! now Im really a tigging!!!
    By welderdude in forum TIG Welding (GTAW/GTAW-P)
    Replies: 8
    Last Post: 07-01-2012, 01:53 AM
  3. Replies: 2
    Last Post: 05-27-2012, 03:21 AM
  4. Forum database fixed.
    By everlastsupport in forum Everlast Announcements, Contests and Promotions
    Replies: 10
    Last Post: 02-07-2011, 02:47 PM
  5. Spool Spool / Roll Adaptor for Power IMIg250P, DYI
    By Ray in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 3
    Last Post: 08-10-2010, 07:46 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •