    When using my spool gun it seems the "spot and stitch" functions don't work. I was hoping to combine the two to improve my mig welding aluminum. Before I start troubleshooting, are these features normally inhibited when using the spool gun???
    Thanks,
    Pete

  2. #2

    Default

    The features are controlled on the panel. Never tried it with the spool gun. Spool gun on that model is controlled on the panel.

  3. Default

    Quote Originally Posted by performance View Post
    The features are controlled on the panel. Never tried it with the spool gun. Spool gun on that model is controlled on the panel.
    Hi Mark,

    I'm going to fool around with it a bit more. I'm having very good luck using .023 wire at 600ipm on my aluminum fixes and want to see about using parts of spot/stitch function to help more.
    Thanks,
    Pete

Similar Threads

  1. IMig 200 For Sale
    By SeanMurphy265 in forum Buy, Sale or Trade
    Replies: 2
    Last Post: 04-03-2013, 12:02 AM
  2. Anyone Tig Welding with an Imig?
    By Kendall in forum TIG Welding (GTAW/GTAW-P)
    Replies: 6
    Last Post: 02-09-2013, 04:58 AM
  3. Magnets and IMig don't Mix
    By Kendall in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 4
    Last Post: 01-24-2013, 06:18 AM
  4. IMig 200 First Welds
    By Kendall in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 18
    Last Post: 01-13-2013, 01:29 AM
  5. power IMIG 205
    By Wrenchtamer in forum Customer Testimonials
    Replies: 3
    Last Post: 03-04-2011, 12:47 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •