    since arc stick welding is doesnt provide good looking welds im wondering if i could take my coiled mig welding unit and plug it into the 200lx i have and use it along with what ever gas i need for either alum or steel welding has any one tried that i think that would work great any thoughts or advices would be helpful

  2. #2

    Default

    brit,

    The Tig/Stick process is CC or constant current. The current stays the same at a given setting, but the arc voltage varies as the length of the arc changes.

    The Mig process is CV or constant Voltage. The voltage remains constant and amperage is controlled or managed through the wire speed. Technically the amps go up the faster the wire is fed because the stickout generally increases.

    I am not sure what you mean by a "coiled" mig gun. Are you referring to a spool gun? The spool gun is also CV.

    Now with that said, you can buy voltage sensing wire feeders that automatically regulate the wire speed if the unit is to be run off of CC power supplies. It isn't a great solution, but it does generally offer satisfactory results when CV isn't available. These type units are used on engine driven welders and typically have a switch that will go from CV to Voltage Sensing depending upon the type of power supply. But they are more than the price of a new mig usually, even used they are quite expensive. If you have one though, it should work fine. Just watch duty cycle issues. I'd suggest our Power I MIG 160 with a spool gun. It does have a stick function and can get by with scratch start tig if needed. Its compact and portable and the price is right!!

  3. #3

    Default

    Quote Originally Posted by performance View Post
    brit,

    The Tig/Stick process is CC or constant current. The current stays the same at a given setting, but the arc voltage varies as the length of the arc changes.

    The Mig process is CV or constant Voltage. The voltage remains constant and amperage is controlled or managed through the wire speed. Technically the amps go up the faster the wire is fed because the stickout generally increases.

    I am not sure what you mean by a "coiled" mig gun. Are you referring to a spool gun? The spool gun is also CV.

    Now with that said, you can buy voltage sensing wire feeders that automatically regulate the wire speed if the unit is to be run off of CC power supplies. It isn't a great solution, but it does generally offer satisfactory results when CV isn't available. These type units are used on engine driven welders and typically have a switch that will go from CV to Voltage Sensing depending upon the type of power supply. But they are more than the price of a new mig usually, even used they are quite expensive. If you have one though, it should work fine. Just watch duty cycle issues. I'd suggest our Power I MIG 160 with a spool gun. It does have a stick function and can get by with scratch start tig if needed. Its compact and portable and the price is right!!
    ok ive bought the 200 lx ac dc stick welder and the 50 amp power plasma cutter from you and so whats your best price for this 160 amp mig unit and will it weld over quarter inch steel and alum

  4. #4

    Default

    Brit,
    email me your email address and what you need. I will get back to you ASAP

  5. #5

    Default hello

    ive tried to contact u by email and phone but no replies about ur best offer for a i mig 160 since i ve bought a powertig200lx and a powerplasma 50 from u already and i want to know if it will weld at least a bit over a quarter inch steel stainless steel and alum and my pager email is balbertson@sprint.blackberry.net and my text is 919 394 5307 thanks

  6. #6

    Default

    Sorry Brit,

    I did find your email, I had made a note to reply but I will work on a reply for you. But as far as a call, I do not have any record of it.
    the I-MIG 160 will be good for 1/4" though, but that will depend just like anything else upon conditions and skill.

Similar Threads

  1. wanting to buy stick welder
    By johnson697 in forum Stick Welding (SMAW)
    Replies: 4
    Last Post: 09-07-2017, 08:05 AM
  2. Power I Mig 200 MIG STICK WELDER , how high should the amp gauge read on stick side
    By Tim L Rogers in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 2
    Last Post: 01-22-2016, 05:42 AM
  3. stick welder aluminum
    By jimmy in forum General Welder Questions
    Replies: 6
    Last Post: 05-25-2013, 06:45 AM
  4. Mystery Welder Revealed: 2012 DIGITAL POWERTIG 210EXT TIG/STICK welder
    By performance in forum Everlast Announcements, Contests and Promotions
    Replies: 46
    Last Post: 07-28-2012, 03:19 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •