I was welding with my 325EXT in triangular wave and the most I could get it to weld was 176 Amps I tried single phase the same as three phase 176 Amps. So I tried all the rest and the same see list below this what the reading was on the machine. So single phase 240V or 3 phase 240V makes no difference plus or minus 1 or 2 amps is nothing, I thought in 3 phase it would be the higher. Still waiting from Everlast Canada. Now I am using the new E3 tungsten and it works very well and triangular wave work very well upside down on aluminum.

3 Phase
Advance square and it got to 320 Amps
Sine wave it got to 220 Amps
Soft square it got to 209 Amps
Triangular wave it got to 176 Amps
DC it got to 321 Amps

Single Phase
Advance square and it got to 320 Amps
Sine wave it got to 221 Amps
Soft square it got to 208 Amps
Triangular wave it got to 175 Amps
DC it got to 321 Amps