Share
Results 1 to 6 of 6

Thread: weld without water cooler

Hybrid View

Previous Post Previous Post   Next Post Next Post
  1. Default weld without water cooler

    Can I weld using the torch that came with my ex250 without it connected to a water cooler? I will be under 150 amps and will not be welding for long periods of time. thanks

  2. #2

    Default

    Quote Originally Posted by snail81 View Post
    Can I weld using the torch that came with my ex250 without it connected to a water cooler? I will be under 150 amps and will not be welding for long periods of time. thanks
    It's not recommended. The easiest thing to do is get some plastic fittings and tubing at your local home center to adapt the torch water connection to your garden hose. This will be a total loss system where you drain the water away from your shop. It only takes a tiny bit of water to keep it cool. Many commercial shops use this method.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  3. Default

    Quote Originally Posted by zoama View Post
    The easiest thing to do is get some plastic fittings and tubing at your local home center to adapt the torch water connection to your garden hose... Many commercial shops use this method.
    True story. I've done it several times

  4. Default

    Im going to build a cheap cooler. 5 gallon bucket and a pump of some sort.

  5. #5

    Default

    Quote Originally Posted by snail81 View Post
    Im going to build a cheap cooler. 5 gallon bucket and a pump of some sort.
    Keep us posted, maybe a picture or two if you get a change. Zoama
    is right though, garden hose, hose and fittings. What we do.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  6. #6

    Default

    for a super cheap total loss setup get a ice maker kit with long plastic line, adapt in, and let long line evac far away somewhere.

    Barry

Similar Threads

  1. TIG Water cooler
    By labmaster02 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 2
    Last Post: 06-24-2015, 01:53 AM
  2. Water cooler
    By srp in forum General Welding Questions
    Replies: 9
    Last Post: 07-10-2012, 07:05 AM
  3. Water cooler requirements
    By dynasim in forum TIG Welding (GTAW/GTAW-P)
    Replies: 17
    Last Post: 05-21-2012, 03:46 PM
  4. Water cooler
    By hesstx in forum TIG Welding (GTAW/GTAW-P)
    Replies: 29
    Last Post: 11-12-2011, 08:19 PM
  5. DIY Water Cooler
    By acourtjester in forum Other Custom Fabrications
    Replies: 3
    Last Post: 06-10-2011, 02:22 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •