Hello. Hoping Lug weld may chime in.
Was using my 164 two days ago. Utilizing the stick and plasma operations.
Both worked fine for the begining. Was cutting, then welding, and switched back to cut mode. And the torch wouldn't light.
It wouldn't respond at all. Until I released the trigger and it air purged... so I believe the lead was fine.
I ended up shutting it off for 15 seconds. Then turned it back on and it worked fine like before...?
Air pressure was steady 72psi at the back of machine. Was on 30amp 220.
Cutting amps 23.
Worked great after I "reset" it..
Was just wondering if this is a known issue..?
Any updated boards that might be out?
I used to build computers so if there is any parts needing replaced and if it's plug and play type boards I could do it myself.
Thanks!
Sent from my SAMSUNG-SGH-I537 using Tapatalk