  1. Angry PowerArc 200ST and 6010 Electrodes

    Hey guys, I just recently purchased a PowerArc 200ST to practice pipe at home specifically for its ability to run 6010 electrodes. I hadn't had a chance to try it out until a month after I had purchased it. I seem to be experiencing some trouble with it. I tried running the 1/8 6010 5P+ and the 5P but it will just barely run them. I usually hold a pretty tight arc to begin with but in this case I really had to hold it tight and if I lifted so much as an 1/8 it would immediately go out. If you've ever tried to do a open root 6G on pipe you know how frustrating that must have been. Sometimes, especially on the hot pass you have to long arc a bit to spread and flatten out the bead but that is simply not going to be possible with this machine. I does however run 7018 like a champ and 6011 better than 6010 but 6011 does not behave like 6010 nor is it a good idea to practice pipe root pass with because when it comes time to test the 6010 5P+ is going to seem like something totally different. Also, I would like to add that I did in fact try it out on both the dedicated 6010 port as well as the regular one.

    If anyone has had the same experience or is not experiencing this problem with their machine please chime in. I would greatly appreciate knowing if there is something wrong with mine or what needs to be done.

  2. Default

    Man that stinks. Are you sure there isn't a switch to be flipped ?
    6010 needs a bit more voltage to stay lit.. lots of inverter machines have trouble with 6010 for that reason. Is there any difference at all??

    And actually 6011 isn't hardly any different. The only difference is one chemical. And that's to aid for AC use of it. In DC it should run almost identical. Whatever helps the rod run AC may help it stay lit with a lower voltage... I know I didn't help you but I'd just download that manual and read read read about that setting and post... it should have its own dedicated spot inside that manual for proper operation.

    Sent from my SAMSUNG-SGH-I537 using Tapatalk

  3. #3

    Default

    There should not be any switch, just the port on the machine with a mod to the internal inverter circuit. Do you see any difference in the regular and 6010 port?
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  4. #4

    Default

    I need to check mine to see if it will run 6010. there is the stick tig switch but the welding lead should be changed to the 6010 port.

    Thanks Ray

Similar Threads

  1. Replies: 4
    Last Post: 06-29-2019, 09:12 PM
  2. PA 200st
    By Angus in forum Stick Welding (SMAW)
    Replies: 6
    Last Post: 07-24-2016, 12:37 AM
  3. Powerarc 200st
    By wade23454 in forum Pre-sales, Sales and Shipping questions
    Replies: 5
    Last Post: 01-06-2014, 11:00 AM
  4. New PowerArc 200ST
    By sophijo in forum Customer Testimonials
    Replies: 10
    Last Post: 09-20-2013, 12:11 AM
  5. PowerArc 200 with no 6010 port
    By Scooter in forum Stick Welding (SMAW)
    Replies: 22
    Last Post: 04-28-2011, 12:50 AM

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •