  1. Default MTS 211si grounding problem

    To set the stage for my question, I have a new (to me) welding table. For ground connection I cleaned a spot on one of the legs with a grinder and welded a 1-1/2" piece of pipe that I cleaned thoroughly. When MIG welding with the piece to be welded laying on the table, I get a small "tack" weld on the table top. I have tried laying the piece on a length of channel iron and connecting the ground cable to the channel iron. I have connected the ground cable directly to the piece. In every case I can think of I am getting the small "tack" weld. I have checked the nut on the ground clamp itself. I have made sure that the ground clamp is in the "-" connection port. I have checked that the connector block on the inside of the machine is "+". What else can I check? Bad ground cable that should be replaced? Thanks for your help.

  2. #2

    Default

    The "small tack" comes from a poor connection to your work. It has nothing to do with the machine or cable. You could try sanding the whole surface of your welding table to get a better connection to your work. Mill scale, paint or rust on the table or part to be welded could cause your problem.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  3. #3

    Default

    You should always ground direct to your item you are welding. You are indirect grounding and loosing a lot of connection and increasing resistance.

Similar Threads

  1. Quick question about grounding a 250 ex
    By Blaze in forum TIG Welding (GTAW/GTAW-P)
    Replies: 2
    Last Post: 07-21-2016, 11:17 PM
  2. Tig Welding Grounding Bar Copper to Steel
    By cbmkr in forum TIG Welding (GTAW/GTAW-P)
    Replies: 0
    Last Post: 12-12-2012, 05:04 PM
  3. Grounding the work table
    By CraigJ in forum General Welder Questions
    Replies: 52
    Last Post: 06-06-2012, 05:47 AM
  4. HF grounding
    By hesstx in forum TIG Welding (GTAW/GTAW-P)
    Replies: 26
    Last Post: 11-22-2011, 10:36 PM
  5. Grounding issues on Cut-50D
    By edllorca in forum Everlast Plasma Cutters (PAC)
    Replies: 3
    Last Post: 06-12-2009, 02:09 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •