"Some" soot is ok..& unavoidable...What you see I caused.....Notice the soot bands on top side of welds...Because of faulty argon flo..AND i wasn't holding the gun 90 degrees..You have sooting on the top side of both..hardly any at the bottom....5356 shuld spray at those numbers...your always gona have to "tweak" it a little...Wire feed is on the panel with the 200....remote function is only with MTS units..An I think the 250 & up..class machines...Didn't get to the point of inductance..gun smoked just as I was dialing in....Im not worried about the gun...In my exp..Everlast has takin care of ALL(all 2)..my equip issues..Yea..Only 2 in 4 years I think...Big deal....LOL...Here's lincoln 5P+++ & tractor supply 1/8 7018..An .023 hard wire..Click image for larger version. 

Name:	IMG_1405.jpg 
Views:	709 
Size:	136.9 KB 
ID:	13425