Thread: 100 PSI argon flo?????

Hybrid View

Previous Post Previous Post   Next Post Next Post
  1. Default 100 PSI argon flo?????

    After playing with the (flawless)steel mig & stick functions..the 200n arrived...set up..acetone THEN new ss wire brush in one direction...21.5 v..355 ipm..25cfh argon....Nothing but turds.....up & down the v wfs thing....same...checked argon fittings with soapy water...all good..took the feed tube out looking for crude in the port...nothing...diffuser clean...check flo but really weak....finally..back to 21.5 v..355 ipm..(my settings at work)..cranked argon up to 60 cfh.....WAY better....crank it wide open...NOW its spraying....great cleaning lines...no soot.......Which leads me to believe..Theres a restriction OR leak starting from the barb on the machine up to the gun......Any 200 dual/200N owners exp this....????...Mark...Ram..Zoama..

  2. #2

    Default

    Quote Originally Posted by stretch View Post
    After playing with the (flawless)steel mig & stick functions..the 200n arrived...set up..acetone THEN new ss wire brush in one direction...21.5 v..355 ipm..25cfh argon....Nothing but turds.....up & down the v wfs thing....same...checked argon fittings with soapy water...all good..took the feed tube out looking for crude in the port...nothing...diffuser clean...check flow but really weak....finally..back to 21.5 v..355 ipm..(my settings at work)..cranked argon up to 60 cfh.....WAY better....crank it wide open...NOW its spraying....great cleaning lines...no soot.......Which leads me to believe..There's a restriction OR leak starting from the barb on the machine up to the gun......Any 200 dual/200N owners exp this....????...Mark...Ram..Zoama..
    I have a similar problem. I think my 200n sucks air through the wire feed tube. Maybe blowing smoke back through it will show the problem. After getting aggravated with mine a few months ago I hung it on the wall and haven't touched it since.
    When I shine a light up the nozzle I can see light around the slits at the back of the nozzle. I wish there was different neck to fit it. I don't like that type nozzle at all.
    Last edited by zoama; 05-21-2016 at 06:10 PM.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  3. Default

    Click image for larger version. 

Name:	20160521_135454(1).jpg 
Views:	620 
Size:	133.3 KB 
ID:	13421Found my problem Zoama....I hooked my steel whip up and pulled the trigger...almost blew my wig off....TONS a argon flo...Hooked the spool gun back up an heard the wind coming from euro connector....The barbed connector from the gas line had burnt(as in melted..lol) from the main stub on the euro...gta bare wire in there too........From the Get go it wasnt shielding...once i went WFO on the argon..it welded sweet for 4 beads...My nozzle is the same...I pulled the ring forward..and the diffuser body blocked the rest of the suction issue as I saw it.....This bites...My machine is rock solid....My gun ???All I needs the barb fitting and forward to fix my deal.....Mark...Got some spare spool gun parts???lol
    Last edited by stretch; 05-21-2016 at 07:28 PM.

  4. #4

    Default

    Quote Originally Posted by stretch View Post
    Click image for larger version. 

Name:	20160521_135454(1).jpg 
Views:	620 
Size:	133.3 KB 
ID:	13421Found my problem Zoama....I hooked my steel whip up and pulled the trigger...almost blew my wig off....TONS a argon flo...Hooked the spool gun back up an heard the wind coming from euro connector....The barbed connector from the gas line had burnt(as in melted..lol) from the main stub on the euro...gta bare wire in there too........From the Get go it wasnt shielding...once i went WFO on the argon..it welded sweet for 4 beads...My nozzle is the same...I pulled the ring forward..and the diffuser body blocked the rest of the suction issue as I saw it.....This bites...My machine is rock solid....My gun ???All I needs the barb fitting and forward to fix my deal.....Mark...Got some spare spool gun parts???lol
    I just opened my euro connector and it looked fine other than a zip tie mashing the argon tube almost flat.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  5. Default

    Quote Originally Posted by zoama View Post
    I just opened my euro connector and it looked fine other than a zip tie mashing the argon tube almost flat.
    LOL...Imagine that.....Thank god my machine not like this......

  6. #6

    Default

    Quote Originally Posted by stretch View Post
    LOL...Imagine that.....Thank god my machine not like this......

    Could you please post a pic or two of your aluminum welds with the 200n so I'll have something to compare mine to?
    I got a few usable welds with 4043 but I can't run 5356 at any setting.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  7. Default

    OK..After stellar support from Andrew..The SG200 is back in action...Put in the new connector & rewired it .. .035 4043 lincioln...040 tip..21,5 & 360 (my start at work) 30/35 cfh......1/4" plate...First pull of the triigger.....It's real close...LOL..amazing what shielding gas will do....lmaoClick image for larger version. 

Name:	20160605_090116.jpg 
Views:	509 
Size:	141.5 KB 
ID:	13431 I'll send more pics when I get it rollin....

  8. #8

    Default

    Quote Originally Posted by stretch View Post
    OK..After stellar support from Andrew..The SG200 is back in action...Put in the new connector & rewired it .. .035 4043 lincioln...040 tip..21,5 & 360 (my start at work) 30/35 cfh......1/4" plate...First pull of the triigger.....It's real close...LOL..amazing what shielding gas will do....lmao I'll send more pics when I get it rollin....
    If you use any 5356 a picture of that along with settings would help me get motivated.... thanks.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  9. Default

    Click image for larger version. 

Name:	20160605_142240.jpg 
Views:	500 
Size:	147.9 KB 
ID:	13432
    Quote Originally Posted by zoama View Post
    If you use any 5356 a picture of that along with settings would help me get motivated.... thanks.
    OK Z...21,3...393...035 5356... .040 tip....35/40 cfh

Similar Threads

  1. Why 100% Argon or Argon/CO2 75/25%
    By mdennis in forum General Welding Questions
    Replies: 6
    Last Post: 08-09-2013, 04:11 AM
  2. Air/Argon
    By ChadP in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 11
    Last Post: 02-09-2013, 09:20 PM
  3. Argon/Air Fittihg
    By NRM in forum TIG Welding (GTAW/GTAW-P)
    Replies: 13
    Last Post: 08-07-2012, 12:39 AM
  4. What is 95/5 Argon/Oxygen gas used for???
    By Brian Ski in forum General Welding Questions
    Replies: 2
    Last Post: 03-22-2012, 05:01 PM
  5. ARGON and ARGON/CO2 TANK SIZES
    By everlastsupport in forum Technical Bulletins and Tips
    Replies: 47
    Last Post: 10-13-2011, 05:19 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •