Share
Results 1 to 3 of 3

Thread: aluminum welding with mig

Hybrid View

Previous Post Previous Post   Next Post Next Post
  1. Default aluminum welding with mig

    Hi All
    need a little help, looking for a mig welder that can weld flux core and aluminum(need to be able to aluminum weld 1/8" channel together on the back corner) preferably 110 or a 110/220 welder

    Thank you for your input

  2. #2

    Default

    The IMIG200 is a good choice. Lots of power for the price. We do aluminum with it all the time. You will need a straight argon tank for aluminum and a CO2 mix for steel (or flux core) if you want to do both. I really would plan on 220volts though.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  3. Default

    Can you get a smooth liner? Does anyone have any experience pushing aluminum through the 10ft gun on these machines? I have heard of using 5053 wire in a larger size and drilling out the contact tip a bit oversize so as to accommodate some thermal wire growth. The 5053 wire seams to have better column strength. I would like to set my I-MIG 205 up for aluminum, but not use a spool gun.
    I MIG 205
    Power TIG 250EX
    POWER PLASMA 60S
    LINCOLN EAGLE 10000
    HOBART HANDLER 135 MIG WELDER
    HF BANDSAW,DRILL PRESS,TORCH SETS,GRINDERS, BELT SANDER
    NORTHERN TOOL DRYCUT SAW
    RONG-FU MILL DRILL
    LINCOLN POWERMIG 256
    1963 SURE WELD 350 AMP STICK WELDER I love this machine and the butter smooth arc 

Similar Threads

  1. mig welding aluminum
    By Rodsmachineshop in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 3
    Last Post: 06-20-2012, 12:50 PM
  2. tig welding aluminum with a DC only tig
    By rab in forum General Welder Questions
    Replies: 18
    Last Post: 04-03-2012, 03:25 AM
  3. My best welding so far... Aluminum... Pic
    By CGCINC in forum TIG Welding (GTAW/GTAW-P)
    Replies: 12
    Last Post: 11-27-2011, 10:36 PM
  4. Replies: 2
    Last Post: 08-03-2011, 04:50 PM
  5. Tig welding aluminum
    By Tallguy64 in forum General Welding Questions
    Replies: 6
    Last Post: 04-11-2010, 12:02 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •