    Today while welding 16ga. Aluminum after I took a short break I started burning thru way to easy. After a little trouble shooting I found that the pedal some how reversed. When I fully depress the pedal it's minimum amps, when the pedal is first pressed its maximum amps. It is a stock 47ohm pedal, AC, 2T, min upslope, min down slope, no pulse. Please help!
    99 jeep tj, almost ready for 1 tons and 40s!

  2. #2
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Take the pedal apart and inspect it. I'm thinking you might have slipped the belt and forced the pot past it's stops or something. You can check the pedal with an ohmmeter if you have one.
    Long arc, short arc, heliarc and in-the-dark!

  3. #3

    Default

    Pins 3-4-5 where 4 is common. Search pinout on the forum, most are list somewhere.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  4. #4

    Default

    I ran a test on the pot. It goes from 1.6-37800 ohms in both directions with no gaps. I tried my digital meter but turns out it doesnt read high enough, so I used my old old analog meter. The switch (pin 1&2) gets continuity when the pedal is depressed. So I put everything back together and tested at the plug and got the same results. Plugged the pedal back in to give it a try hoping maybe the belt slipped a tooth but now at the very beginning of pedal travel it has to low of amps to create a stable arc. Push it alittle further and I get an arc, and it ramps up until mid pedal and then amps start going down until the end of pedal travel. Immediately pulled the plug and ran a test and got the same 1.6-37800 in both directions.
    99 jeep tj, almost ready for 1 tons and 40s!

  5. #5
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    From what you describe, it really sounds like a bad pot. Actually analog meters are usually better than digital for testing them as you can see if the response curve is smooth and even. But even then you won't be testing under load, so some things can still not show up. I would just replace the pot, as an easy test. If you have a 47K pedal, the reading you are getting is out of spec, anyway. Most pots are no more than 10% tolerance. You could also measure the control and output voltages, as the pot is usually running as a variable voltage divider.
    Long arc, short arc, heliarc and in-the-dark!

  6. #6

    Default

    yeah I'm thinking your right. It's about the only thing that would cause the kind of changes I'm seeing. Plus it is far from 47k. I assume I can order these through everlast? Or maybe I might just upgrade pedals.
    99 jeep tj, almost ready for 1 tons and 40s!

  7. #7
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Pedal upgrade you can get from them, or direct from SSC.
    https://www.ssccontrols.com/product/c950-0725/
    The replacement pot you will probably have to source yourself. Digikey, Mouser, Amazon, ebay, local electronics store, etc.
    Long arc, short arc, heliarc and in-the-dark!

  8. #8

    Default

    great! thank you for all your help!
    99 jeep tj, almost ready for 1 tons and 40s!

  9. #9

    Default

    So it took awhile but I finally got my new SSC pedal. Unfortunately the machine is still doing the same thing. low amps at start, max amps at mid travel and low amps at full pedal. Beginning acts like hf doesn't want to work. Tested ohms on pedal and it's doing what it's suppose to.
    99 jeep tj, almost ready for 1 tons and 40s!

  10. #10
    Join Date
    Mar 2012
    Location
    Remote S. Idaho
    Posts
    53

    Default

    Quote Originally Posted by Rambozo View Post
    Pedal upgrade you can get from them, or direct from SSC.
    After owning an ST-205 for about five years with a foot pedal that's never worked right, I came here this morning to ask if the SSC unit works. Thanks. I'll order one now.
    There is no safe direction to point an unsafe gun.
    PowerPro 205
    Hobart 250HF
    Powcon 300ST
    gas stuff
    14x60 Hercules Ajax lathe
    Gorton I-22 MastrMil
    Landis 6x18 surface grinder
    20" Powermatic bandsaw
    Ancient, big drill press
    350 pound anvil and a bunch of hammers
    If I can't fix it I can make it.....unrecognizable.

Similar Threads

  1. powerpro 256 pedal problem ?
    By cdale2002 in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 4
    Last Post: 05-30-2014, 04:42 AM
  2. Wireless pedal for PowerPro 256?
    By ScottRussell in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 1
    Last Post: 12-01-2012, 05:38 PM
  3. Problem with foot pedal on LX 225
    By brianscott in forum TIG Welding (GTAW/GTAW-P)
    Replies: 11
    Last Post: 06-23-2011, 05:44 PM
  4. foot pedal problem
    By johnson697 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 1
    Last Post: 12-17-2010, 03:06 PM
  5. superultra 205 foot pedal problem
    By agrrob in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 3
    Last Post: 10-31-2010, 11:42 AM

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •