    So, I have been welding on some sheet metal lately its all 14ga steel and have been supplied a Lincoln 140hd with .035 Fluxcore wire and its just not an attractive weld at all. It burns through super easy no matter the settings and am considering the use of 1/16" 6013 electrodes instead of wirefeed. It's either that or get a smaller fluxcore wire as its a very windy area. Thoughts? I suppose running the welder off 100ft of 120v extension cord isn't helping any either but no choice for that.

  2. #2
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    In the past I did a lot of sheet metal with 6013. I think it works fine, but you might also try 7014. I think you will like the results a lot better than fluxcore, except for the speed.
    Long arc, short arc, heliarc and in-the-dark!

Similar Threads

  1. Power I Mig 200 MIG STICK WELDER , how high should the amp gauge read on stick side
    By Tim L Rogers in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 2
    Last Post: 01-22-2016, 05:42 AM
  2. 14 gauge sheetmetal tig ballpark ??
    By braveops in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 5
    Last Post: 11-13-2013, 05:36 AM
  3. Brazing/Soldering Galvanized Sheetmetal - techniques?
    By jakeru in forum General Welding Questions
    Replies: 20
    Last Post: 10-03-2011, 10:02 PM
  4. Project 1 form Revkev6: 1932 ford sheetmetal pinhole repairs
    By revkev6 in forum On Road Fabrication
    Replies: 0
    Last Post: 08-29-2011, 12:17 AM
  5. Aluminum sheetmetal shroud for under-mounted Horizontal Bandsaw motor
    By jakeru in forum Other Custom Fabrications
    Replies: 2
    Last Post: 05-08-2011, 06:07 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •