Share
Results 1 to 12 of 12

Thread: New consumables

Hybrid View

Previous Post Previous Post   Next Post Next Post
  1. Default New consumables

    For the past six months we have been working on bringing the best quality line of Consumables for our Plasma Tig Mig Products.
    Given the huge amount available over the internet and other places this may seem at first to be a simple project.
    However it is not as simple as it first apeared. After gathering samples from various Suppliers we narrowed our search to a short list of suppliers. The only problem with samples is it does not tell you how consistent the production is going to be. Any one can sort through a pile of cons and send the best of the batch to you. With this in mind our next step was to pop in to the potential suppliers with very little advance notice.Everytime i went to visit our Welding Factory i would take the time to visit those company,s that we where interested in . Some where a far cry from what we expected and fortunately for us our new Supplier far exceeded our expectations.
    There where a number of points that really impressed me . The facility for manufacturing was one The updated CNC machines used for producing the parts . The organised Warehouse facility for Finished products The quality procedures that where actually followed ( there are lots of ISO Factory,s but it only works if you follow the procedure and not fudge the books for Auditing )And one other point that really impressed me was the Raw material used is imported from Finland and Domestic materials are not used. ( too high a tin content in domestic )
    A lot of people may think why bother consumables are just consumables and there is no difference from getting them from Ebay / Harbour Freight etc
    But for us it is just one more way we can supply the best product to our customers to bring out the best performance for all our units.
    With this in mind we will now be having the E laser etched on Nozzles tips etc.
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	Consumables for site 015.jpg 
Views:	509 
Size:	84.2 KB 
ID:	358   Click image for larger version. 

Name:	Consumables for site 017.jpg 
Views:	489 
Size:	82.9 KB 
ID:	359   Click image for larger version. 

Name:	Consumables for site 019.jpg 
Views:	497 
Size:	83.5 KB 
ID:	360   Click image for larger version. 

Name:	Consumables for site 028.jpg 
Views:	495 
Size:	84.0 KB 
ID:	361   Click image for larger version. 

Name:	Consumables for site 030.jpg 
Views:	518 
Size:	78.7 KB 
ID:	362  

    Click image for larger version. 

Name:	Consumables for site 026.jpg 
Views:	499 
Size:	91.9 KB 
ID:	363   Click image for larger version. 

Name:	Consumables for site 027.jpg 
Views:	506 
Size:	96.3 KB 
ID:	364   Click image for larger version. 

Name:	Consumables for site 033.jpg 
Views:	546 
Size:	99.0 KB 
ID:	365  
    EVERLAST CANADA
    www.everlastwelders.ca
    www.titanwinches.com

    905 637 1637

  2. Default great explanantion

    I enjoy hearing why the consumables you sell are of a certain quality. In purchasing my unit never once did I see any cheap substandard anything. Everlast offers a 5 yr warranty which tells me a lot. Love my 256 thanks

  3. Default

    Looks good but do they last longer than the old ones?

  4. Default

    The new consumables do in fact last longer than our previous product .
    This is readily apparent when just using them while testing units. Trying to get wear marks on the electrode tips to show the Torch has been tested took a lot longer than with our old Cons. In fact we ended up dragging the tip to get a burn mark on the electrode to show it had been used as our conventional method was really not showing any wear on the electrode.
    I wanted the E placed on them to distinguish our product due to the fact that it is simple enough to get any Welding Consumable that you can imagine but for the most part they are the same quality and have the same imperfections .
    I am not sure if a camera can pick up the imperfections but i will take some pictures and see if the differences can be seen just to show why i believe we have a Superior line of Consumables from previous .
    EVERLAST CANADA
    www.everlastwelders.ca
    www.titanwinches.com

    905 637 1637

  5. #5
    Join Date
    Jul 2010
    Location
    In the Land of CoRn
    Posts
    69

    Default

    I was in the local welding supply store looking for consumables, and they stated "we don't sell Chinese junk." So I flipped over the tungsten they almost sold me and showed him the "made in China" sticker.

    I looked at harbor freight, they didn't have any plasma cutter consumables that looked remotely close to what is on the cutting torch on the 256. What amazed me is they had 3" pre-sharpened tungsten though!

    It would be nice to be able to pick something up locally in a pinch though.

    The laser etching is a nice touch!

  6. #6

    Default

    Tell them to show you a product they sell that doesn't have a made in china label on it....

Similar Threads

  1. Consumables
    By rkinken in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 11
    Last Post: 03-25-2016, 02:57 PM
  2. Where are you getting your consumables?
    By Klr49adv in forum General Welding Questions
    Replies: 9
    Last Post: 12-04-2013, 06:21 PM
  3. TIG consumables
    By Rambozo in forum TIG Welding (GTAW/GTAW-P)
    Replies: 18
    Last Post: 08-19-2012, 08:11 PM
  4. Consumables
    By weildkorp in forum Everlast Plasma Cutters (PAC)
    Replies: 3
    Last Post: 02-23-2010, 09:12 PM
  5. Consumables
    By CapnMilo in forum General Welder Questions
    Replies: 6
    Last Post: 02-10-2010, 06:47 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •