Quote Originally Posted by pavetim View Post
Yeah I usually have a big fan blowing it out since it's flux core I can have good airflow. I was using Lincoln ER70S-6 with 80/20 Argon/CO2 and holy #### the spatter I was getting. I know it's mostly the galvanizing causing the spatter but I'm going to try some different wires anyways. Plus holy #### does this Lincoln wire grind hard, it's taking me longer to grind all the seams out smooth than it is to do the whole project. Hoping the silicon bronze wire works out, I heard it grinds real nice. It's just a powder coating oven so really just filling in the seams for the sheet metal.
Try holding a tighter arc (shorter stickout). With flux core you can take the nozzle off to see better. Did you switch polarity for flux core ?