    Looking for info on which spool gun works with the power mig 275s. The SM200N or SM200 MTS? I have two SM200N guns.
    Everlast PowerTig 250EX w/ PowerCool W300
    Everlast PowerMig 275S
    Everlast PowerPlasma 60S

  2. #2

    Default

    SM200MTS is supposed to work with it. The 200N standard does not have amp control in the gun handle. You have to control it on the panel. The MTS does have amp control in the handle.

  3. Default

    Performance,
    Thanks for the info. But will the sm200n work with it? I had a I mig 250 which had to be controlled at the panel so that's OK, just need to know if they will work with the 275s. Thanks.
    Everlast PowerTig 250EX w/ PowerCool W300
    Everlast PowerMig 275S
    Everlast PowerPlasma 60S

  4. #4

    Default

    No. It won't. Not designed to.

  5. Default

    Ugh. Now I have to see how to get another issue taken care of. Thanks
    Everlast PowerTig 250EX w/ PowerCool W300
    Everlast PowerMig 275S
    Everlast PowerPlasma 60S

Similar Threads

  1. New Power Mig 275s- First use findings.
    By Blaze in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 13
    Last Post: 08-23-2017, 05:02 AM
  2. Power i MIG 275S Manual and other new manuals
    By performance in forum Everlast Announcements, Contests and Promotions
    Replies: 1
    Last Post: 08-17-2016, 04:28 AM
  3. Power i-MIG 275S video
    By Rambozo in forum Everlast Announcements, Contests and Promotions
    Replies: 1
    Last Post: 07-20-2016, 07:45 PM
  4. Why can't I add a spool gun to my TIG?
    By performance in forum Welding articles from Professionals (knowledge database)
    Replies: 11
    Last Post: 07-21-2011, 09:12 PM
  5. Spool Spool / Roll Adaptor for Power IMIg250P, DYI
    By Ray in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 3
    Last Post: 08-10-2010, 07:46 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •