Share
Results 1 to 6 of 6

Thread: First Actual Aluminum TIG Project With 210EXT

  1. Default First Actual Aluminum TIG Project With 210EXT

    Yes, even though I’ve had my 210EXT for 8 month or more, I’ve only used it for projects with mild steel, maybe a little stainless too. I mean, I’ve done some practice aluminum beads, but didn’t want to waste much Argon doing practice.

    Click image for larger version. 

Name:	Gearbox copy.jpg 
Views:	1131 
Size:	61.1 KB 
ID:	13314

    Anyway, a fun little project emerged that I almost defaulted to my mild steel mentality, but instead decided to used some aluminum collars to come up with a much improved motor mounting solution for a surprisingly powerful and well-priced eBike mid-drive system.

    Click image for larger version. 

Name:	Motor5 copy.jpg 
Views:	1104 
Size:	75.0 KB 
ID:	13315 Click image for larger version. 

Name:	Motor3 copy.jpg 
Views:	1088 
Size:	66.0 KB 
ID:	13316

    I’ll post photos here, and link to a video on it, where it shows me using 210EXT briefly, at about 10-12 minutes in.

    Click image for larger version. 

Name:	Motor4 copy.jpg 
Views:	1040 
Size:	54.5 KB 
ID:	13317 Click image for larger version. 

Name:	Motor6 copy.jpg 
Views:	1035 
Size:	65.8 KB 
ID:	13318

    Feel free to offer any critique, as I’m not a TIG expert. Most will notice that the AC frequency is at around 200.


  2. #2

    Default

    Good, creative solution. You might want to contact the company and show them this and they might even send you some proto types to test if they work it out.

  3. Default

    Hey, thanks for that nice feedback, Mark,

    Yeah, the company/importer I bought the kit/system from (Luna Cycle) recently started an eBike forum that I participate on, so they know about my little "build" and many others that are spontaneously emerging as threads there. But they might be taking a note already.

    http://electricbike.com/forum/forum/...r-etrike-build

    Quote Originally Posted by performance View Post
    Good, creative solution. You might want to contact the company and show them this and they might even send you some proto types to test if they work it out.
    Last edited by christian; 03-16-2016 at 06:57 PM.

  4. Default

    Well, here's my "Second Actual Aluminum TIG Project With 210EXT".

    Yeah, it has to do with he same Cyclone eBike Mid-Drive project though. Much like the aluminum collar mounts for the motor were a first for my aluminum welding of an actual project, this battery box is the second, and was surprisingly challenging. I mean DC TIG welding of a mild steel battery box for my other 2WD trike project was a breeze (it's painted silver, not aluminum).

    Click image for larger version. 

Name:	MildSteel Box.jpg 
Views:	1006 
Size:	80.2 KB 
ID:	13330

    I mean, even on the mild steel box, I ground down the beads to make it look cleaner, as welds look like Frankenstein to me, unless they're all identical in their bead profile throughout a project, and I'm not that good. So, anyway, I was a little surprised at how much trickier the aluminum battery box was to do. It came out well, and I ground down all of the beads but one of the better ones, to show as a reference.

    Click image for larger version. 

Name:	BeadProfile.jpg 
Views:	979 
Size:	59.1 KB 
ID:	13331

    Anyway, I think my 210EXT welder did well, as it tended to give me that thin bead profile that I was seeking, by using the Triangle wave at 200 Hz. But, still, technique seems much more critical on aluminum, with things like torch angle. Maybe it was the thinness of the 16 gauge metal itself, or the 3003 alloy. Whatever, I like it well. Maybe I'll step up the gauge thickness a little next time.

    Click image for larger version. 

Name:	AluminumBox.jpg 
Views:	966 
Size:	56.3 KB 
ID:	13332
    Last edited by christian; 03-27-2016 at 05:45 PM.

  5. #5

    Default

    I'm not well coordinated in dabbing filler and advancing the torch so when building an aluminum box I leave one edge hanging over the other maybe .01" and use no other filler.
    From a computer case that doubles as a air purifier that I built a while back.



    Last edited by zoama; 03-27-2016 at 08:25 PM.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  6. Default

    Hey,

    Thanks for that.


    Quote Originally Posted by zoama View Post
    I'm not well coordinated in dabbing filler and advancing the torch so when building an aluminum box I leave one edge hanging over the other maybe .01" and use no other filler.
    From a computer case that doubles as a air purifier that I built a while back.
    Last edited by zoama; 03-27-2016 at 08:26 PM. Reason: fixed quote code

Similar Threads

  1. My aluminum skiff project.
    By downline in forum Other Custom Fabrications
    Replies: 4
    Last Post: 12-21-2016, 02:50 AM
  2. My Fourth Small Aluminum TIG Welding Project With Everlast 210EXT
    By christian in forum Welding Projects and Pictures
    Replies: 8
    Last Post: 09-13-2016, 02:56 PM
  3. Help with aluminum project
    By Markz in forum TIG Welding (GTAW/GTAW-P)
    Replies: 11
    Last Post: 08-08-2012, 03:39 AM
  4. My first Aluminum project on my 225LX
    By sw2x in forum Other Custom Fabrications
    Replies: 0
    Last Post: 03-03-2012, 11:58 PM
  5. Replies: 0
    Last Post: 06-20-2011, 06:54 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •