Share
Results 1 to 9 of 9

Thread: Foot Pedal Mods

  1. #1

    Default Foot Pedal Mods

    Hi All
    I did some mods to the foot pedal that came with my PM 256. I read that other guys had probems with the timing belt shaft getting off the pot and not working. See attached pictures. I made 2 brackets on of 1/4" X 1" X 1" angle about 1-1/2" long and the other is 1/8" flat cut to shape and bent to a 90.
    I used 10-32 screws and nuts to hold them on. The 1/4" bracket has a tongue that sticks info the back of the timing belt shaft as a guide.

    Have fun
    acourtjester
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	DSCF4101.JPG 
Views:	810 
Size:	65.1 KB 
ID:	243   Click image for larger version. 

Name:	DSCF4106.jpg 
Views:	879 
Size:	88.5 KB 
ID:	244   Click image for larger version. 

Name:	DSCF4109.jpg 
Views:	892 
Size:	86.4 KB 
ID:	245  

  2. #2
    Join Date
    Jan 2010
    Location
    Milton FL Was from San Rafael CA
    Posts
    16

    Default

    Hi acourtjester good idea i took your ideaand brought it up 1 more stage
    the shaft is long and was flexing at the gear i made a nylon block that suports the shaft
    bolted it through the top
    the hole is 1 size over 1/4"
    now it will not dut exesive wear at reastat
    thanks for sparking an idea
    Jim
    Last edited by jandlcars; 01-09-2010 at 10:34 PM.

  3. #3

    Default

    Hey Tom,

    Thanks for posting your mod. It will make the pedal go a long way for sure.

    I saved what you emailed me as well. We should have a new pedal coming soon. Lower profile as well.

    Love to see pics of the Nomad if you ever get time. Have a good weekend.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  4. #4

    Default

    Quote Originally Posted by everlastsupport View Post
    Hey Tom,

    Thanks for posting your mod. It will make the pedal go a long way for sure.

    I saved what you emailed me as well. We should have a new pedal coming soon. Lower profile as well.

    Love to see pics of the Nomad if you ever get time. Have a good weekend.
    no nomad I have a 34 ford???

  5. #5

    Default

    Sorry, wrong fellow, I thought it was you. Heck, 34's Fords are welcome here too.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  6. #6

    Default

    Great idea Tom. I may have to mod mine when I get some time.
    Wayne

  7. #7
    Join Date
    Jan 2010
    Location
    Milton FL Was from San Rafael CA
    Posts
    16

    Default

    Update on Pedal Mod
    after trying it it worked better with nylon block and acourtjester's mod but it still skipped
    after watching the action of the belt had a cam style action
    i took a small spring and bent it to go over the lower belt screw and to the box aprox
    1/2" from the bottom with a 6/32" machine screw
    this light spring keeps it in contact with gear
    spring came from Home Depot tn a package of mixed springs its about 3/16" x 2"

    mike i had a Nomad but its gone was in original shooting in the back ground of american Grafetti it is not in cut version
    i have a 1925 t truck street rod i built in the 70's
    Jim

  8. #8
    Join Date
    Dec 2009
    Location
    Greater Seattle, WA
    Posts
    813

    Default

    I've got one of the first Everlast Super200P's. I do remember making some mods to the footpedal.

    Mine arrived a bit torqued, (maybe from shipping maybe was put together that way.) The main thing I did was fix that, so the frame was square, and I removed some play in the hinge (I added some bronze bushings on each side.) I got the toothed rack nice and square, and tight with the pot gear also, so that should work well for a long time.

    Also I used a multimeter, to test the range of the min (which is when the microswitch engages) to max, when the footpedal maxes out, and I made some adjustments that extend the range. I can weld with the footpedal as low as 10 amps. I think pressed down, I get pretty close to 200 amps, just a bit under. My footpedal is made of steel, and has a knob on the side. Its held up well.

  9. Default

    Lower profile would be great. Since there's so little to the whole peddle, I think making it the size of a sewing machine foot peddle would be much more comfortable. That big foot peddle is way too hard to press when you're sitting down.
    Charlie

    Everlast 225 LX
    Everlast PP 50

    HF 130 TIG/90 ARC
    HF 90 fluxcore

    ATX MIG (don't ask)

Similar Threads

  1. 250 EX Foot pedal
    By Dick Eue in forum TIG Welding (GTAW/GTAW-P)
    Replies: 5
    Last Post: 09-27-2018, 04:49 PM
  2. Foot pedal mods for PA160-STH
    By joshuab in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 21
    Last Post: 08-21-2013, 05:43 PM
  3. Foot Pedal Fix
    By Ron66 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 1
    Last Post: 03-26-2012, 12:29 AM
  4. new foot pedal
    By hesstx in forum TIG Welding (GTAW/GTAW-P)
    Replies: 2
    Last Post: 12-16-2011, 05:26 PM
  5. Bad foot pedal?
    By sth212 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 6
    Last Post: 08-21-2011, 08:50 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •