My Everlast machine is a powerpro 205 which I've had since new, I've been doing pretty good with my beads on mild steel with the TIG process and I've gotten pretty good with the Plasma cutting. however, today I just tried the machine on aluminum and it was a total disaster. The machine was set to AC, AC balance was set at 90%, 5 liter per minute on the argon, using # 5 gas lens. I think the problem was with the 1/16" electrode at 100 amps trying to run a bead on 1/8 aluminum. Within 5 seconds the electrode disapeared into the cup like a huge ball, I sharpened the electrode , reinstalled it, turned the amps down to about 75 and the same thing happened. I really think the problem is the thinner electrode to say the least and I do not think its a fault with the machine since its usually user error when things go wrong.. I wish there was a troubleshooting section for this somewhere on this forum. What did I do wrong ? help