    Default Fixing a $1.00 Chinese measuring cup with $5.00 of Safety-Silv 56

    What can I say? I liked the measuring cup and didn't want to see it repurposed outside the kitchen.

    Photo number one is after brazing with oxy acetylene and a Harbor Freight version of the Smith mini torch. I *should* have tinned each part then held the two together with a spring clamp heating until the brazing compound liquefied again. It would have made for a cleaner joint with less goopy edge. Oh well, next time.

    The second photo is after cleaning with a Scotch-Brite pad on a die grinder following up with the Dremel and buffing compound.


    Click image for larger version. 

Name:	A.jpg 
Views:	273 
Size:	138.5 KB 
ID:	13306
    Click image for larger version. 

Name:	B.jpg 
Views:	280 
Size:	140.2 KB 
ID:	13307

  2. #2

    Default

    Quote Originally Posted by fyidiy View Post
    What can I say? I liked the measuring cup and didn't want to see it repurposed outside the kitchen. Photo number one is after brazing with oxy acetylene and a Harbor Freight version of the Smith mini torch. I *should* have tinned each part then held the two together with a spring clamp heating until the brazing compound liquefied again. It would have made for a cleaner joint with less goopy edge. Oh well, next time. The second photo is after cleaning with a Scotch-Brite pad on a die grinder following up with the Dremel and buffing compound. Click image for larger version. 

Name:	A.jpg 
Views:	273 
Size:	138.5 KB 
ID:	13306 Click image for larger version. 

Name:	B.jpg 
Views:	280 
Size:	140.2 KB 
ID:	13307
    Looks good to me. Hey if you like someone thing and have the tools to do it. A project and some fun. What size if the cup. Looks small.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  3. #3
    Join Date
    Aug 2014
    Location
    Westerville, Ohio
    Posts
    72

    Default

    The size is 1/2 cup.

Similar Threads

  1. fixing a railcar
    By jerky in forum Welding Repairs
    Replies: 16
    Last Post: 08-17-2012, 11:44 AM
  2. Bit confused on the chinese connection....
    By Mike J in forum TIG Welding (GTAW/GTAW-P)
    Replies: 5
    Last Post: 12-16-2011, 05:24 PM
  3. safety...
    By aaxiss in forum Forum related Questions
    Replies: 14
    Last Post: 05-10-2011, 12:25 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •