  1. Default

    Quote Originally Posted by rick9345 View Post
    Empty questions like this beg a smart answer.

    now give the forum some real info on the problem

    I have been welding with the tig process for 10 years solid, the high frequency is not starting the arc correctly. Regardless of settings or process DC/AC the arc doesn't start correctly. Never had a problem with any other machines.

    Using foot pedal.

    It's not an empty question, it's a question in what to check to fix a hi freq arc initiation problem that isn't setting or operator based. What info are you looking for? It's a question that also states all settings / parameters and consumables have already been checked. And we are looking for some assistance in tracking down a mechanical issue with the machine.
    Last edited by zoama; 02-29-2016 at 11:51 PM. Reason: Please be nice

Similar Threads

  1. PP256 High-Freq. wont turn off!!!
    By tensecond408 in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 5
    Last Post: 03-07-2014, 09:12 PM
  2. Starting an arc
    By Effinay in forum TIG Welding (GTAW/GTAW-P)
    Replies: 9
    Last Post: 05-23-2012, 02:34 AM
  3. Starting a new cut mid way
    By trickbiker in forum Everlast Plasma Cutters (PAC)
    Replies: 4
    Last Post: 01-16-2012, 09:25 PM
  4. 250 ex Arc starting
    By trackmaster in forum Customer Testimonials
    Replies: 3
    Last Post: 10-21-2010, 04:40 PM
  5. PM 256 Hi-Freq quit working
    By Tony_F in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 8
    Last Post: 08-19-2010, 09:12 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •