    Yeah,

    I'm not an old pro like Sage Hill with AC TIG, but I've had the lower-output EXT unit (210), as your/his new 255EXT. And though I haven't tried welding aluminum cans together, I do think the AC arc gets stable pretty quickly beyond its 5 amp starts on the Square wave, i.e. around 20 amps or less, with about 30% AC balance, a sharp tungsten, and around 120-200 Hz on AC frequency. The Triangle wave seem pretty cool for a finer bead too. Of course, AC TIG still seem noisy to me, compared to the calm and quiet DC TIG arcs. Also, I'm liking the 5356 filler rod better than 4043.

    Please let us all hear how it goes with your new 255EXT, as I'm diggin' my 210EXT, but maybe can learn some new settings that you will discover, which could make it even better for me too.

    Hey, look, the EDIT feature on the Forum here seems to work fine again. Maybe things here on the Forum are pretty good again. Whee...!
    Last edited by christian; 02-14-2016 at 09:35 PM.

Similar Threads

  1. What is Your Pre-Flow Setting
    By NRM in forum TIG Welding (GTAW/GTAW-P)
    Replies: 4
    Last Post: 08-09-2012, 01:57 AM
  2. AC / DC Setting is backwards?
    By JonS in forum TIG Welding (GTAW/GTAW-P)
    Replies: 3
    Last Post: 05-02-2012, 02:25 AM
  3. Pulse Setting in AC
    By Buggy Chief in forum TIG Welding (GTAW/GTAW-P)
    Replies: 1
    Last Post: 03-30-2012, 11:25 AM
  4. 250EX Amp Setting Changes??
    By CMB in forum TIG Welding (GTAW/GTAW-P)
    Replies: 8
    Last Post: 08-11-2011, 03:13 AM
  5. Pulse setting of PM 205
    By www in forum TIG Welding (GTAW/GTAW-P)
    Replies: 5
    Last Post: 08-05-2010, 10:32 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •