    Hi all. New guy here

    Been reading over new purchase 250EX manual and says don't use pure tungsten (don't have any) and no 1% Zirconiated.(I just bought $60 worth of 2 sizes) ouch.

    Question is... why, and are there any other "NO's" for Inverters? Wanting to weld on 1/16" to 3/8" Mild steel, Alum. and Stainless before it's all over. Also nice to know if there is "this is always works better" advice". Again, my first Inverter welder. Thanks in advance.

  2. #2

    Default

    2% lanthanated works well for everything. 3/32 size will cover most welding. Best price I've found http://www.weldingcity.com/tig-tungs...0-lanthanated/
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  3. Default

    ABN TIG Tungsten Electrodes 2% Lanthanated Blue 10 Pack 3/32"x7" (2.4mm x 175mm)

    https://www.amazon.com/dp/B00OPE42JW..._S7eMwbQVPVWAR

  4. #4

    Default

    I'm with Zoama. 2% lanthanated and I use weldingcity.com. I see the amazon post, probably fine too. Do not get a lot of welding supplies from amazon, but the seem to have everything else.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  5. #5

    Default

    Thoriated is common and it is not a bad choice. Among the best starts with any tungsten.

  6. Default

    OK! Quick response. Making me glad to be on this site. Haven't done a lot of welding other than backyard stuff with MIG and some TIG in a class room. saw many good posts on this Everlast 250EX so took the plunge. Reading manual got me concerned about applications and consumables with this inverter.

    I agree about the Lanthanated and have a good supply of it. BUT! that Zirconiated was recommended for the very thin metals for better arc start, which I will be getting into directly and can't afford screwing up this machine investment. I do take a warning seriously when it is in the manual.

    I'll keep scouring this site for more insight and again...great forums and thanks for having me.

Similar Threads

  1. running 250ex off inverter
    By carking2320 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 1
    Last Post: 04-01-2015, 12:48 PM
  2. Inverter generator use for powering welders
    By sportbike in forum TIG Welding (GTAW/GTAW-P)
    Replies: 22
    Last Post: 09-29-2013, 04:38 AM
  3. Replies: 11
    Last Post: 10-15-2011, 05:29 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •