Well,
"LPM" may be a problem. 10 LPM is about 20 CFH, I believe, which is high for 70 amp, I think. But it also sounds like you have your AC balance backwards. And the Miller and Lincoln units do read opposite, I believe.
I'll bet there's no issue with the machine. When I first got my 210EXT about 6 months ago, I had a momentary issue with HF starts, and even called Everlast Support, which was probably Mark that I spoke to, and the issue was resolved in two minutes, as it had to do with a machine setting and too high a flow of Argon on a necked-down cup, as I was using lowered amps. I mean, I kept welding, with just scratch starts until I got the call back from my message 15 or 20 minutes earlier.
Since that time I've never looked back, so to speak, and think the 210EXT is best TIG welder in it's class on planet Earth.