Share
Page 2 of 3 FirstFirst 123 LastLast
Results 21 to 40 of 45

Thread: Tig newbie questions

  1. #21

    Default

    Use the darkest shade that allows you to see your puddle clearly.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  2. Default

    Thanks for the tips. All set now. To practice that is....

    New helmet work perfect.

    Very first and second tig weld




  3. Default

    was looking at more flexible smaller torches. was looking at this one. http://weldfabulous.com/ck-ck17-12-r...-fx-superflex/

    will it use all the consumables i have now that came with my new tig 200DX? I believe its a 26 torch

    or do i have to get all new consumables for this 17flex?

    do i have to get a cable connector? not sure which one

  4. #24

    Default

    Everlast sells everything CK, just call sales. 26 and 17 use the same consumables.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  5. Default

    Talked to everlast canada. Dont deal with ck at all

    Cant seem to find anyone in canada for ck torches

  6. #26

    Default

    You should be able to get one from the US with no problems. I'd stay clear of ark zon.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  7. #27
    Join Date
    Mar 2011
    Location
    Eastern Oregon
    Posts
    681

    Default

    I'd stay clear of ark zon.
    Any particular reason?
    Penncrest Buzzbox - Infinite amp control! Man the 70's were good.
    Everlast Powerplasma 60 - Reliable unit, cuts well.
    Everlast i-MIG 250P w/spoolgun - Really smooth, plenty of cajones.
    Everlast 250EXT - Sometimes it just takes a kick in the balls...
    Everlast 255EXT - Just started playing

  8. #28

    Default

    I have been happy with weldingcity. Sounds like Zoama might have got a bad deal from AZ.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  9. #29

    Default

    I learned a lot about them when I bought my second CK torch. The owner told me a ridiculous number of lies including "your order has been delayed for one week because the employee handling your order is taking a week vacation". Speaking with the CEO of CK cleared up a lot of things and made it much easier for people to buy CK products on the internet without any BS. IMO the zone guy is mentally ill... blew up my email with lies, apologizes, threats and begging (like a child having a tantrum). He even went so far as to put a line in his many emails stating that the emails were for my eyes only and sharing or forwarding them would bring legal action. Maybe he's changed his ways... I certainly hope so. Honesty is the best policy.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  10. Default

    i narrowed it down to one or both of these


    1. CK 17 superflex

    CK17-12-RSF FX (150A, 12.5ft Superflex cable, flex head)

    #SL2-35QD (1/2” Dinse w 12” gas hose quick disconnect for CK9, CK17)



    2. Trimline 26 Torch

    TL26-12-RSF FX (200A, 12.5ft Superflex cable, flex head)

    #SL8-35QD (1/2” Dinse w 12” gas hose quick disconnect for CK26, TL26)

  11. #31

    Default

    I recommend a #9 size for the majority of welding under 150 amps (ck9 or ck130) and a ck 26 or 210 for the heavy stuff.
    The cable on those 200 amp gas cooled torches is heavy compared to the one used up to 150 amp. The smaller cable feels like a shoe string in comparison.
    Here's an old post where I compared my torches http://www.everlastgenerators.com/fo...1164#post31164
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  12. #32

    Default

    Even though the ck130 is rated for 130 amps, that rating is at 100% duty cycle both AC/DC. It can run at 150 amps or a little more for shorter runs like 5 minutes or so. Lower quality #9 torches are rated at 125 amp 60% duty cycle only in DC and rated for just 80 amps AC. Duty cycle is percentage of ten minutes the torch can handle rated amps. CK says 100% means non-stop. Torches get much hotter in AC than DC.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  13. #33
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    The perfect torch really depends more on the kind of work you are doing. Hard to beat a superflex #9 for light work and thinner material, shorter duration welds.
    For any extended aluminum work, water cooled is the only way to go. In between those two is where the 17 and 26 live. Also depending on if you are welding at a bench or are more mobile, can change things, like air or water cooled and lead length. While 12' is usually fine at a bench, 25' will let you move around a garage or a larger project, without having to drag the machine around.
    Long arc, short arc, heliarc and in-the-dark!

  14. Default

    How thick can u weld with the ck 9 torch?

  15. #35
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by calltrex View Post
    How thick can u weld with the ck 9 torch?
    It depends on for how long. 1/4" steel for small things, 1/8" almost continuously, but the torch will get a bit hot to handle, so you will probably take a break from time to time to give it a chance to cool off. It's great for repairs or for tacking up large projects, but for continuous duty I find it a bit lacking.
    What kind of things are you welding?
    Long arc, short arc, heliarc and in-the-dark!

  16. Default

    Quote Originally Posted by Rambozo View Post
    It depends on for how long. 1/4" steel for small things, 1/8" almost continuously, but the torch will get a bit hot to handle, so you will probably take a break from time to time to give it a chance to cool off. It's great for repairs or for tacking up large projects, but for continuous duty I find it a bit lacking.
    What kind of things are you welding?
    mostly just little brackets or whatever in my garage. prob mostly aluminum now. thats why i got a tig to do aluminum. 3/16, 1/8

    looks like the CK17 is a better all round option. and if i have to do thicker stuff i can use the 200amp torch that came with machine.

    also ck17 and 26 can use the same parts

  17. Default

    done deal now. ordered the CK 17 superflex and flex head

    still need to get the stubby lens kit from everlast. way cheaper then from CK

  18. Default

    CK 17


  19. Default

    Torch came today. so much nicer and light and smaller

    good for most of my projects.

    for big stuff ill have to use the original 200 amp torch

    im sure ill replace that one with the trim line superflex torch kit later
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	20160108_165907 copy.jpg 
Views:	798 
Size:	145.3 KB 
ID:	13193  
    Attached Images Attached Images  

  20. Default

    Pics don't show up properly in this forum






Similar Threads

  1. Newbie with a Tig
    By slanwar in forum General Welding Questions
    Replies: 7
    Last Post: 02-11-2018, 11:10 PM
  2. Okie newbie
    By iaokie in forum Introduce Yourself
    Replies: 2
    Last Post: 05-17-2017, 12:15 PM
  3. Newbie MIG Welder
    By fotoa in forum Introduce Yourself
    Replies: 4
    Last Post: 08-12-2015, 09:16 PM
  4. Old Newbie
    By Lone Wolf in forum Introduce Yourself
    Replies: 9
    Last Post: 01-08-2012, 08:25 PM
  5. newbie from pennsyltuckey
    By kingoftopsoil in forum Introduce Yourself
    Replies: 0
    Last Post: 08-15-2010, 05:27 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •