  1. Default tig torch defect alert!

    I was trying my 2016 250ex out today for the first time on tig and I put a 3/32 tungsten in the torch head. I happen to notice that the back cap that clamps the tungsten in place was not letting the O-ring seal against the torch body. The tungsten was clamping before the O-ring was inside the head. I had to chuck all the collets that came with the machine up in my lathe and cut about 3/32 of an inch off the back part of the collets. I ordered a gas lense kit from ebay and all the collets that came with that kit were already shorter so they would seal. Any of you that have been having trouble with shielding better look at the collets.
    Miller 302 gas drive
    millermatic 200 mig
    miller spoolmatic 3 spool gun with 100ft ext.
    2014 Everlast PP60S plasma
    thermal arc 250 GTS inverter
    2016 Everlast 250EX
    miller tig cooler
    2015 Everlast MTS250S
    Miller 30A spool Gun
    Miller xtreme 12VS wire feeder
    Linde CM 85 shape cutter

  2. Default

    Thanks for posting! I had a similar issue. The oring would seal, but barely. I decided to follow your advice by shortening the collet and it fits much better now.

  3. #3

    Default

    At worst that would be a collet defect not a "torch defect".
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  4. Default

    Quote Originally Posted by zoama View Post
    At worst that would be a collet defect not a "torch defect".
    I stand corrected
    Miller 302 gas drive
    millermatic 200 mig
    miller spoolmatic 3 spool gun with 100ft ext.
    2014 Everlast PP60S plasma
    thermal arc 250 GTS inverter
    2016 Everlast 250EX
    miller tig cooler
    2015 Everlast MTS250S
    Miller 30A spool Gun
    Miller xtreme 12VS wire feeder
    Linde CM 85 shape cutter

  5. #5

    Default

    No,
    Neither would be a defect. There are always a couple of extra threads cut into the collet body threads. If you screw them all the way up, then they will do that. Our torches are not unique in that as I've seen it in other brands. Leave it a little loose and it will all work fine.

  6. Default

    Quote Originally Posted by performance View Post
    No,
    Neither would be a defect. There are always a couple of extra threads cut into the collet body threads. If you screw them all the way up, then they will do that. Our torches are not unique in that as I've seen it in other brands. Leave it a little loose and it will all work fine.
    If that is not a defect I do not know what a defect is. I have been on this forum for about 2 years, not once has this been brought up on any of the threads about people having problems with shielding. It does not matter who else is having the problem, if it is known it should have been addressed. I have been welding all my life and I have had jobs where almost all I do is tig weld and I have never come across this problem before ever. Call it what ever you want it is still a problem and I am sure more than one has blamed their machine and spent wasted time searching for what is wrong.
    Miller 302 gas drive
    millermatic 200 mig
    miller spoolmatic 3 spool gun with 100ft ext.
    2014 Everlast PP60S plasma
    thermal arc 250 GTS inverter
    2016 Everlast 250EX
    miller tig cooler
    2015 Everlast MTS250S
    Miller 30A spool Gun
    Miller xtreme 12VS wire feeder
    Linde CM 85 shape cutter

Similar Threads

  1. 160STH defect with foot pedal
    By DrivenToMake in forum TIG Welding (GTAW/GTAW-P)
    Replies: 7
    Last Post: 08-12-2017, 01:33 AM
  2. Floating head Machine Torch holder w/ S45 Machine Torch - 2 for sale.
    By countryguy in forum Everlast Plasma Cutters (PAC)
    Replies: 2
    Last Post: 12-19-2016, 09:52 PM
  3. Change tig torch to a smaller water cooled torch
    By wheelrdealer in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 4
    Last Post: 09-18-2012, 04:07 PM
  4. Model 26 Torch & General Torch Questions...
    By Ray C in forum TIG Welding (GTAW/GTAW-P)
    Replies: 14
    Last Post: 08-26-2012, 03:47 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •