    AC will create a tone at the frequency the machine is set for. The arc directly vibrates the air like a Tesla coil. Also the arc length has an effect as that causes the voltage to change. A long arc length will be louder. In theory you could modulate your weld frequency with music and the arc would play a tune while you're welding. Not very practical, better to use hearing protection when doing AC TIG , especially over an extended time. You will get a similar effect when using hi frequency pulse settings on DC.
    Long arc, short arc, heliarc and in-the-dark!

  3. Default

    The 255EXT manual Highly Recommends wearing ear protection while using high AC frequencies and high pulse.

  4. Default

    OK, thanks, I'm not hallucinating! Ha, ha, ha...

  5. Default

    Gee, maybe I was hallucinating, as I ran a few beads on the same piece of aluminum tubing today and it seems quieter somehow. I mean, nothing like DC quiet of course.

  6. #26

    Default

    Change the frequency or the wave form and the sound will be a different pitch and a different decibel level.

    It can be more than uncomfortable to listen to at times.

  7. Default

    Yeah, I think that's what it was. I was trying all the wave forms and speeding up the Hz frequency to 250.

    Man, I'm really diggin' this 210EXT. And I think I'm settling on the typical square wave at 120HZ for the moment. I won't be doing too much aluminum, but I dig being able to add another material to projects, beyond stainless steel, that is able to give an unpainted, brushed finish and be lighter too.

    I'm likin' that CK SteadyGrip hand amptrol with it also.

    Rock On, Everlast staff!

  8. #28
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Long arc, short arc, heliarc and in-the-dark!

  9. #29

    Default

    Good stuff Rambozo.

    Happy Thanksgiving to all!
    Everlast 250EX with cooler and WP20 Torch
    Millermatic Mig Welder
    Gas welding setup
    A bunch of Snap-On tools
    And a Brain

Similar Threads

  1. Cooling fans
    By Toby in forum TIG Welding (GTAW/GTAW-P)
    Replies: 30
    Last Post: 07-02-2013, 04:02 PM
  2. Hello fellow Everlast fans from KY
    By n4in in forum Introduce Yourself
    Replies: 1
    Last Post: 12-07-2011, 10:38 PM
  3. Did you DIY your water cooling system?
    By DaveO in forum TIG Welding (GTAW/GTAW-P)
    Replies: 55
    Last Post: 05-03-2011, 08:11 AM
  4. Fittings on pp256 torch cooling lines
    By haveissues in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 7
    Last Post: 04-10-2011, 07:45 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •