    When I saw the 2016 version of the PowerTIG 250EX was available, I ordered one. I haven't used the machine yet, but the quality over my older 200DX is night and day! I was really surprised how much Everlast has stepped up their quality on this machine.

    How I received the box. I was pulling on the white straps, but they were where they were supposed to be when I picked it up.



    Box of goodies:




    The hose is way better than my old one:



    Foot pedal:



    The torch lead was covered in a sleeve. Very nice! Even though I haven't used the torch, I will even with my CK torch. This torch looks so much better, I just have to try it out.



    The case:
    Purple Fabricator 211i

  2. #2

    Default

    The case:






    Control panel.







    Once I use the machine, I'll post some video.

    Thanks!
    Purple Fabricator 211i

  3. Default

    Nice I am am at the same place you are. I got my new 250ex 2 weeks go but All I have had time for is to unbox it. I need to modify cart I have to mke it fit . Then I will give it a go. It looks like it will be another week or so before I get to use it.
    Miller 302 gas drive
    millermatic 200 mig
    miller spoolmatic 3 spool gun with 100ft ext.
    2014 Everlast PP60S plasma
    thermal arc 250 GTS inverter
    2016 Everlast 250EX
    miller tig cooler
    2015 Everlast MTS250S
    Miller 30A spool Gun
    Miller xtreme 12VS wire feeder
    Linde CM 85 shape cutter

  4. #4
    Join Date
    Oct 2015
    Location
    Washington, THE STATE!
    Posts
    9

    Default

    Mine came in last week. I got it up and running Saturday and could not believe how nice it really was. I bought it to learn How to TIG Aluminum. Works Great so far!

  5. #5

    Default

    This welder is for sale. Never used it. 0 hours on it.

    It will come with the aftermarket pedal, and also a CK torch.

    $1000 + shipping.

    email me James@CaptainHooligan.com

    Local pickup in Asheville, NC or PayPal
    Purple Fabricator 211i

Similar Threads

  1. Brand new, never used 2016 PowerTIG 250EX
    By 225 in forum Buy, Sale or Trade
    Replies: 1
    Last Post: 08-30-2016, 02:29 AM
  2. Just got my PowerTig 250EX 2016
    By Speedy112790 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 10
    Last Post: 04-30-2016, 01:41 AM
  3. 2016 250EX AC stick welding
    By TheGary in forum Stick Welding (SMAW)
    Replies: 5
    Last Post: 12-13-2015, 08:39 PM
  4. 2016 250EX vs 210EXT
    By Steve-H in forum Pre-sales, Sales and Shipping questions
    Replies: 3
    Last Post: 10-08-2015, 02:51 PM
  5. 2016 PowerTIG 250EX
    By 225 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 1
    Last Post: 10-01-2015, 08:24 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •