    I needed a set of shelves to keep the clutter off my tables and for extra storage. They are 6' tall 4' wide and 2' deep on 5" total lock stem casters.
    The square tubing is 1"x1"x1/8" and 16ga sheet metal for the shelves. All 90' of tubing was cut precisely with my Evolution Rage 3 DB cold saw. The sheet metal was plasma cut.
    I weld a 1/2"x13tpi nut inside the bottom of each upright for the caster to thread into. The 8 hangers on the sides are 1/2" round bar, all bent at the same time in my press brake.
    All joints welded spray arc with the 250p because it's almost silent and spatter free. The sheet metal was tacked every few inches with TIG and no filler.
    I'll give it a coat of Rustoleum 9100 black epoxy mastic sometime this week. Maximum weight capacity is 1200lbs.

    Click image for larger version. 

Name:	1.jpg 
Views:	1188 
Size:	144.7 KB 
ID:	13093Click image for larger version. 

Name:	2.jpg 
Views:	2022 
Size:	146.5 KB 
ID:	13094Click image for larger version. 

Name:	3.jpg 
Views:	1166 
Size:	147.1 KB 
ID:	13095
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  2. #2
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,662

    Default

    Looks nice. What was your gas blend for that?
    Long arc, short arc, heliarc and in-the-dark!

  3. #3

    Default

    Quote Originally Posted by Rambozo View Post
    Looks nice. What was your gas blend for that?
    I made a quick coupling tee and mix my c25 with straight argon. I ran 4 lpm c25 and 8 lpm argon, .035 wire and a 1/2" nozzle, 24v but I don't know the wire speed. I lit up on a piece of scrap and turned it down until it sprayed right. I thought about making it a cabinet but decided to just keep it shelves.

    Click image for larger version. 

Name:	4.jpg 
Views:	2070 
Size:	146.6 KB 
ID:	13096Click image for larger version. 

Name:	5.jpg 
Views:	2080 
Size:	146.6 KB 
ID:	13097
    Last edited by zoama; 09-23-2015 at 02:42 AM.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  4. #4

    Default

    Quote Originally Posted by Rambozo View Post
    Looks nice. What was your gas blend for that?

    What gas blend do you use for spray transfer ?
    Last edited by zoama; 09-25-2015 at 06:04 AM. Reason: typo
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  5. #5
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,662

    Default

    Quote Originally Posted by zoama View Post
    What gas blend do you use for spray transfer ?
    Usually 98/2 Argon/O2. The shop I used to be next door to, used some kind of inhouse triple blend that worked great, but they are no more, and I don't know what the blend was.
    Long arc, short arc, heliarc and in-the-dark!

  6. Default

    Quote Originally Posted by Rambozo View Post
    Usually 98/2 Argon/O2. The shop I used to be next door to, used some kind of inhouse triple blend that worked great, but they are no more, and I don't know what the blend was.
    LWS around here sells what they call trigas or trigon (something like that) that is a 3 gas blend. I used it years ago but do not remember much about it. I think Airgas sells it too.
    Miller 302 gas drive
    millermatic 200 mig
    miller spoolmatic 3 spool gun with 100ft ext.
    2014 Everlast PP60S plasma
    thermal arc 250 GTS inverter
    2016 Everlast 250EX
    miller tig cooler
    2015 Everlast MTS250S
    Miller 30A spool Gun
    Miller xtreme 12VS wire feeder
    Linde CM 85 shape cutter

  7. #7

    Default

    Here is an interesting read on shielding gas and marketing snake oil. http://www.weldreality.com/MIG_welding_gases.htm Read the whole page please.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  8. #8

    Default

    Quote Originally Posted by TheGary View Post
    LWS around here sells what they call trigas or trigon (something like that) that is a 3 gas blend. I used it years ago but do not remember much about it. I think Airgas sells it too.
    Prax has stargon. My son likes is over c25. Do not recall what the third gas was (O maybe?). I rarely deal with Prax and Airgas. We are very lucky to have WSI (welder services inc). Always use Mitch, never does me wrong. We had a small shop (Lake welding) the were good but too far to drive,

    Nice shelves by the way.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

Similar Threads

  1. Heavy duty I beam welding question.
    By Brian Ski in forum General Welding Questions
    Replies: 3
    Last Post: 05-25-2012, 04:27 AM
  2. Tank rolling ???
    By Rodsmachineshop in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 4
    Last Post: 04-28-2012, 12:30 PM
  3. Project 1 from DaveO (210 Ext contest): shelf repair
    By DaveO in forum Welding Repairs
    Replies: 0
    Last Post: 02-07-2012, 11:53 AM
  4. CGCINC Project#6: 1962 Flair stove rolling cart
    By CGCINC in forum Hobyist Projects
    Replies: 19
    Last Post: 01-09-2012, 03:13 AM
  5. Trailer mods for winch and gas/cooler shelf
    By chadford in forum Other Custom Fabrications
    Replies: 0
    Last Post: 07-08-2011, 06:15 PM

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •