Thx. Yes, I've printed the online manual. It only has a brief section on the plasma function. I've used the unit a lot for TIG welding. There is a loose screw on the ground clamp. But it's held tightly the spring. Re the swirl ring, must it be right side up? I could not find a good picture of its proper orientation. Looks the same to me either side up.