    The welder I had previously was a simple 200 amp DC welder and everything was going decent but I wanted to upgrade to the 250EX.That's where the problems started.
    Using the same bottle of argon and electrode as before I now can't reliably start an arc with DC. The weird part is that I can start the arc on the old welding table, on a piece of stainless steel laying on the table and on a piece of copper, the arc in the copper is dead stable, on the stainless a little less so and a little strange on the table with long arcs that appear to come almost from the collet. The only way I can reliably start an arc on the stainless piece that I'm attempting to weld is to warm the electrode by starting an arc on the copper and then quickly moving to the part.
    The pieces I'm working on are freshly machined and washed down with acetone and I've gone so far as to clamp the ground directly to the part. I've tried from 10 - 20 cf argon, base current at 140 and using the foot pedal or lower and the torch switch. The electrode seems to have an etch right up to the collet from the starting arc.
    I'm not blaming the welder yet, the last time I used a welder with half the capabilities of this one, the first Apple computer had just come on to the market, any idea what I have done ?
    Last edited by zoama; 08-22-2015 at 01:04 PM. Reason: Title said XE instead of EX

  2. #2

    Default

    Post a clear picture of the welder so we can see the settings, please.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  3. #3

    Default

    And the collet and weld/material.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  4. Default

    I don't think I need to preface this with 'I'm not a welder, but' these are the settings I used as well as others. I tried using the torch trigger, both 2T and 4T, and the foot pedal 2T only.

    Click image for larger version. 

Name:	20150822_110219.jpg 
Views:	588 
Size:	113.4 KB 
ID:	13078Click image for larger version. 

Name:	2015-08-22 11.01.49.jpg 
Views:	607 
Size:	81.8 KB 
ID:	13079Click image for larger version. 

Name:	2015-08-22 11.00.54.jpg 
Views:	942 
Size:	88.8 KB 
ID:	13080

  5. #5

    Default

    Verify that argon is flowing out of the cup.
    Have the tungsten about 1/8" from the material to be welded.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  6. Default

    Definitely is argon and it's 'clean' argon, I was using it with the last welder and it worked well. The old welder was a very basic Chinese 200 amp DC welder and it worked. I was thinking that I had something wrong but what is confusing to me is that it works very well on the copper but almost not at all on my part. The other thing that I found strange was that the HF start was almost like a 1920s or 30s movie where they had 20 foot lightning bolts. One time when it started there was a white smoke that came out of the torch when I tried to initiate an arc as well. Is it possible the torch is NG?

  7. #7

    Default

    Anything is possible but I haven't seen a bad torch on one of these. I'm gonna have to leave this one to the tech support guys but I'm sure it'll be something simple.
    Tech support normally works monday through friday but may show up on the weekend from time to time.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  8. Default

    Thanks anyway, I'm in Canada so I'll give Duncan a call when I return from vacation.

Similar Threads

  1. 250ex problems
    By Draino in forum TIG Welding (GTAW/GTAW-P)
    Replies: 7
    Last Post: 06-20-2015, 07:22 PM
  2. 250ex arc problems welding on ac but not dc ?????
    By slufoot2005 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 11
    Last Post: 10-12-2013, 02:48 PM
  3. 250EX problems with foot pedal
    By Boosted P in forum TIG Welding (GTAW/GTAW-P)
    Replies: 20
    Last Post: 03-09-2012, 03:51 AM
  4. New 250EX owner, a few problems
    By Adambomb in forum TIG Welding (GTAW/GTAW-P)
    Replies: 109
    Last Post: 03-18-2011, 03:11 AM
  5. shipping problems with new 250ex?
    By Bulldad3 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 4
    Last Post: 02-28-2010, 02:37 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •