Share
Results 1 to 5 of 5

Thread: imig200

Hybrid View

Previous Post Previous Post   Next Post Next Post
  1. Default imig200

    I've said this on several other venues but I want to add a comment in the testimonial area. I bought an imig 200 a couple of years ago and modified it to use a Miller 30A gun. The original concept was a machine that can run aluminum for the times I'm called for a small job that is remote. This is not a shop machine as the duty cycle is to low but for my purposes it has been outstanding. Mind you, it has the stones to weld 1/2" material at its top end but you really have to watch the time. The arc quality is very good with AL wire and on stick, frankly, it is one of the best welders I've ever used using 3/32 rod. In one load I can pack the welder, gun and extension cord. The 2nd load is the argon cylinder.

  2. #2

    Default

    Quote Originally Posted by Yofish View Post
    I've said this on several other venues but I want to add a comment in the testimonial area. I bought an imig 200 a couple of years ago and modified it to use a Miller 30A gun. The original concept was a machine that can run aluminum for the times I'm called for a small job that is remote. This is not a shop machine as the duty cycle is to low but for my purposes it has been outstanding. Mind you, it has the stones to weld 1/2" material at its top end but you really have to watch the time. The arc quality is very good with AL wire and on stick, frankly, it is one of the best welders I've ever used using 3/32 rod. In one load I can pack the welder, gun and extension cord. The 2nd load is the argon cylinder.
    I have many machines 255EXT 210EXT 250P, 205P, PP50, PP80, etc. All great machine, but the IMIG200 was always a favorite if you read many of my posts. We kept it for aluminum mainly with a spool gun on it. If you stay in the duty cycle, this machine will not let you down. And the light weight and able to run on a 5500 watt generator makes you a mobile welder. If you take CO2 type tanks, do not lay them on their side. Mobile aluminum you can lay the argon tanks flat.

    Had to chime in as this is one of my favorite machines. I bought mine for my youngest son to start with years ago.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  3. #3
    Join Date
    Oct 2012
    Location
    Canada, Suttonwest, Ontario
    Posts
    676

    Default

    I am back for a few day and then back on the road again for a few more weeks I only used a IMIG200 once and it work quit well but you still can't find a better all-round machine then the MTS250S and it work very well with a Miller 30A Spool gun thanks to Yofish to make it work with the 30A.
    Everlast PowerTig 325EXT (Canada)
    Everlast Power I Mig 250 (Canada)
    Everlast PowerPlasma 80S (Canada)
    Everlast PowerCool W300 (Canada)
    Everlast PowerMTS 250S Fitted with a 30A Spoolgun(Canada)
    Miller Dynasty 400 wireless(Canada)
    Millermatic 252 plus 30A Spoolgun(Canada)

  4. #4

    Default

    I'm no electronic guru but, I do know the amp of the breaker has something to do with the duty cycle of the Imig 200. When I used mine on a 30 amp breaker I could bump the duty cycle. I carried it to a friend's shop and welded all day on a 50 amp breaker; I never hit the duty cycle, & that was the most I had used that machine in one day.
    Lincoln Eagle Engine Drive
    Everlast MTS 250
    Everlast Power Tig 225lx
    HTP Mig 2400
    Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
    Miller Spectrum 375 Extreme Plasma cutter
    Victor cutting torch
    HF 20 Ton Shop Press
    HF 4x6 Band Saw
    HF Air Compressor
    Northern Tool Drill Press


    www.murphywelding.com

  5. #5

    Default

    The newer model IMIG200 has more power than the older model. We've had both, the old one would run on the 5500 Porter Cable no problem (180-190 amp range from the welder). New model, the generater would strugle at max amps (volts). So a 5500 is a little small and that is in the 25-27amp range +/-. So it is right on the line at 30 amps, or was for us. I have a PC 10000 but too heavy to move around. I like the new model better, but the old one paid for itself many times over and mobile was nice.

    Also, I have seen breaker go bad (get weak). We lost a 50amp dedicated to a welder.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

Similar Threads

  1. wire feed speed Imig200
    By stretch in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 14
    Last Post: 05-19-2016, 10:48 PM
  2. Imig200 flux core welding questions
    By sw2x in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 17
    Last Post: 03-30-2013, 11:24 AM
  3. Imig200 duty cycle @200amps ?
    By CNC Chris in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 5
    Last Post: 12-07-2012, 03:45 AM
  4. IMIG200- anyone tried Scratch start tig?
    By ogorir in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 9
    Last Post: 06-12-2011, 03:04 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •