					Hope you enjoy your new machine!
I have never MIG welded aluminum, but here is some more feedback based on what I've heard and read. Ordinarily, a MIG machine's feed mechanism grips steel wire inside the machine and pushes it through the cable and out the gun. Aluminum MIG wire is too soft for this setup to work- any bend or resistance in the cable will cause the wire to kink and stop feeding. A spool gun gets around this because the distance from the spool to the contact tip is a few inches, rather than several feet.
As Christian says, you can give it a try, but I suspect you'll ultimately need a spool gun.
				
			 
			
		 
			
				
			
			
				DaveO
Oxweld oxy acet gear
IMIG 200
PowerTIG 210 EXT... Amazing!