    Thanks everone, for the help i think its my pedal been using torch switch like zoama said and seems to work ok. I have an ssc pedal from my lincoln 185 tig that im going to see if ssc company can send me the everlast connector for it and if it will work if not i will buy a new one.
    Thanks again i will keep everyone informed

  2. #2

    Default

    Make sure you have only "pedal" selected. Or make sure you don't have upslope/downslope set to anything but zero. Also make sure end amps are set to minimum value.

  3. #3

    Default

    And clean. clean clean, your work clamp connection (hooking it direct to the metal you are welding as well) and double check to make the cable is tight and clean in the DINSE connector on the work clamp.

  4. #4
    Join Date
    Jul 2015
    Location
    san leandro CA
    Posts
    17

    Default

    Thanks Mark for the reply, the up and down slope is 0 and end amps are as low as it goes and my clamp is tight and grounded good ran multiple passes with the torch switch and it seems like its the pedal, torch switch works good had two start fails on a/c but the arc is alot better and stable than it is with the pedal.

  5. #5
    Join Date
    Jul 2015
    Location
    san leandro CA
    Posts
    17

    Default

    Still having issues on ac side this cant even hold an arc at 5 amps like on dc there is gotta be a problem with the ac side of this machine i bought an ssc pedal and still the arc is horrible shoot out like a flame thrower not always but still the arc is all over not steady like on DC

  6. #6
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    What is your arc length? Too long an arc can give you fits with low amp AC.
    Long arc, short arc, heliarc and in-the-dark!

  7. #7
    Join Date
    Jul 2015
    Location
    san leandro CA
    Posts
    17

    Default

    Its 1/8 to 3/16 it can"t start an arc on 5 amps on ac and has a hard time on most amps once it gets going it works but when you let off on the pedal the arc get all weird i tried a soda can and soon as you step on the pedal it burns right through and its on 5 amps max, dc works fine, on ac it just changes tone and jumps all over and if u let off the pedal the arc continues and dosen't shut off some times not always. just got the SSC pedal but did it with the supplied pedal i think its the machine, tried it with torch switch same thing, on high amps it has a hard time starting the arc and keeping it steady also but no always been doing it sense i got it, even tried it on the factory ac settings that come preset same thing it like it can"t get it going. its frustrating because i know its not me but don't know what it is. Thanks
    Last edited by slzboy; 08-09-2015 at 11:51 PM.

Similar Threads

  1. new 255ext
    By aaron1 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 0
    Last Post: 06-07-2016, 01:37 AM
  2. Advice on new 255ext set up
    By Dedvetpath in forum TIG Welding (GTAW/GTAW-P)
    Replies: 1
    Last Post: 01-01-2016, 02:32 PM
  3. 255ext?
    By redbeard in forum Pre-sales, Sales and Shipping questions
    Replies: 5
    Last Post: 03-26-2015, 09:12 AM
  4. 255ext
    By kafer in forum Pre-sales, Sales and Shipping questions
    Replies: 3
    Last Post: 02-15-2014, 02:11 AM
  5. Replies: 21
    Last Post: 11-21-2012, 11:26 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •