Originally Posted by
zoama
Any luck finding those settings? Do you use different settings for 5356?
The forum has that jumping cursor problem again where midway through typing a sentence the cursor jumps to the line above.
With 4043 .047 it work very well on my MTS 250 V23.2 wire speed and amps 276 100% argon set at 22CFM no smoke nice clean weld on a aluminum .25 and .375.
Everlast PowerTig 325EXT (Canada)
Everlast Power I Mig 250 (Canada)
Everlast PowerPlasma 80S (Canada)
Everlast PowerCool W300 (Canada)
Everlast PowerMTS 250S Fitted with a 30A Spoolgun(Canada)
Miller Dynasty 400 wireless(Canada)
Millermatic 252 plus 30A Spoolgun(Canada)