Quote Originally Posted by zoama View Post
I tig welded my boat stringers with 5356. My spool gun has to be sucking air somewhere because I've been through every setting systematically several times with the same results. It can't be the gas since I use the same bottle for tig.
I haven't been out to the shop for a while since my best friend and fishing partner got out of the fence and was run over and killed by some a-hole who didn't bother to stop.
I have being reading this post on spool gun and aluminum welding on mine it was the gas flow was to low on tig welding at was set to 25 to 30 SCFH @ 50 PSIG for aluminum and had to go to 50 to 55 SCFH @ 50 PSIG for the spool gun to get it to work with 5356 but 4043 does work a lot nicer. Sorry about you fishing buddy, had my buddy for 17 years still miss the old girl after two years had a heart attack, dog have them too.