Share
Page 1 of 2 12 LastLast
Results 1 to 20 of 25

Thread: 325EXT took a dump

Hybrid View

Previous Post Previous Post   Next Post Next Post
  1. Default 325EXT took a dump

    Well, my luck has struck again. Welding along today at 75 amps, DC, no pulse when all of the sudden I couldn't strike an arc. I tried grounding the tungsten to the work repeatedly and nothing, looked over at the machine and the panel is dark with the fan running, WTF!?! Of course this happens when I'm seriously under the gun with work. Called tech support, he said cycle the breaker on the wall, maybe a leg isnt making good contact... well of course that didn't work. No other ideas from tech. Gave me an RA number and said I may could get a board sent to me to try. Two calls in so far, no response. Really really anxious as I've read some horror stories on warranty or service work. The machine is 6 months old, 2015 model, single phase, NOT worked hard at all. Is there any diagnosing I can do myself? I can verify with my meter that theres 240V going to the board at one point, but have no display lights at all and nothing from the gas solenoid when hitting the pedal or switch. Does this seems like a board failure?

  2. #2

    Default

    Quote Originally Posted by WhitsonMetal View Post
    Well, my luck has struck again. Welding along today at 75 amps, DC, no pulse when all of the sudden I couldn't strike an arc. I tried grounding the tungsten to the work repeatedly and nothing, looked over at the machine and the panel is dark with the fan running, WTF!?! Of course this happens when I'm seriously under the gun with work. Called tech support, he said cycle the breaker on the wall, maybe a leg isnt making good contact... well of course that didn't work. No other ideas from tech. Gave me an RA number and said I may could get a board sent to me to try. Two calls in so far, no response. Really really anxious as I've read some horror stories on warranty or service work. The machine is 6 months old, 2015 model, single phase, NOT worked hard at all. Is there any diagnosing I can do myself? I can verify with my meter that there's 240V going to the board at one point, but have no display lights at all and nothing from the gas solenoid when hitting the pedal or switch. Does this seems like a board failure?
    I had one leg burned under a breaker once on my AC... it read 240v every time but when I put a load on it one leg would go away. It's a long shot but I would test the circuit with a different load or pull the breaker to check. You could also check the connections in the plug and at the breaker/power switch in the machine to be sure they have good contact. Hope it's something simple.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  3. Default

    Nah, it's not something simple like that. All the shop wiring is new, tried it on 3 different outlets/breakers just wishing, but no. Theres ONE welder in town I can buy, a Miller Diversion 180, nothing else around. I'd hate to have to buy it but I have a pile of work to do.

  4. Default

    Well, no calls back today. Does anyone have any sort of diagnostic ideas I can try? I'd love it if it was a simple bad solder or something, can't find any troubleshooting info.

  5. #5
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by WhitsonMetal View Post
    Well, no calls back today. Does anyone have any sort of diagnostic ideas I can try? I'd love it if it was a simple bad solder or something, can't find any troubleshooting info.
    As this machine is pretty new, you will most likely have to be the troubleshooting trailblazer. First thing I would do is a through visual inspection of the insides, specifically all board to board interconnects. Then go over the boards to check for obvious physical or thermal damage. If you have electronics knowledge you can trace the low voltage power supply that powers the control boards. Check voltages at the primary filter caps and before and after the voltage regulators. You should be able to look up the data sheets to see if things are in spec. Probably a 5 volt rail for most of it, but it could be 3.3, as a lot of new micros are going that way. Since the display is dark, that's where I would start.

    However, be sure to talk to support to get the OK to proceed. I'm not sure how many of these have been repaired, so they may not have much in the way of statistics on what goes wrong with them, apart from the common shipping damage from being dropped and such. If you are under the gun to finish a bunch of work, it's probably not the right time to try and troubleshoot an unknown machine. Rent or buy a replacement machine. You can always sell it later.
    Long arc, short arc, heliarc and in-the-dark!

  6. Default

    Well, you're right that I shouldn't poke at this thing too much as I don't have an in-depth electrical skill set. This just couldn't have happened at a worse time and while I really need a machine right now, the closest thing is a Dynasty or a Lincoln Aspect. Buying one of those means green is gone as they're both a HUGE investment. Never had a machine go down and man is it throwing me for a loop now.

  7. Default

    Mine is run on single phase 240. If you'll pm me an email address I'll send you the full sized picture.

  8. #8
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by WhitsonMetal View Post
    Mine is run on single phase 240. If you'll pm me an email address I'll send you the full sized picture.
    Both models will run on single phase 240. If you look on the back it should say if the second option is 240 3 phase or 480 3 phase.
    Long arc, short arc, heliarc and in-the-dark!

  9. Default

    Rambozo, here is a shot of the old one. I took it to make sure I got everything plugged back in Click image for larger version. 

Name:	20150721_093604.jpg 
Views:	403 
Size:	164.3 KB 
ID:	13061

  10. #10
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by WhitsonMetal View Post
    Rambozo, here is a shot of the old one. I took it to make sure I got everything plugged back in Click image for larger version. 

Name:	20150721_093604.jpg 
Views:	403 
Size:	164.3 KB 
ID:	13061
    Well it sure looks like there is some type of programming port right next to the processor. Can't make out any chip numbers from that pic, though.
    My curiosity is piqued by the unpopulated sections, where two transformers go. Is this the 240/480 model or the 240 only model? Overall it looks like a nice board layout.
    Long arc, short arc, heliarc and in-the-dark!

  11. Default

    Any updates on your machine? Resolution? Watching threads like this as I consider whether to go with Everlast or a different brand.

  12. #12

    Default

    Quote Originally Posted by Dedvetpath View Post
    Any updates on your machine? Resolution? Watching threads like this as I consider whether to go with Everlast or a different brand.
    Customer is taken care of !
    Last edited by zoama; 07-20-2015 at 07:03 PM. Reason: typo
    Oleg Gladshteyn
    Phone: 650 588 8082 / 877 755 WELD
    Cell: 415 613 6664 ONLY IF YOU REALLY NEED IT
    Email: oleg@everlastwelders.com
    Website www.everlastgenerators.com

    www.linkedin.com/pub/oleg-gladshteyn/48/b08/875

  13. #13

    Default

    I think auto correct messed up the message Oleg was sending. I think somewhere it should have said "customer has been taken care of." Which in long speak I believe means that the customer's unit should have been shipped out.

  14. #14
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by Oleg View Post
    Customer is taken care of !
    Whacked?
    Long arc, short arc, heliarc and in-the-dark!

  15. Default

    Actually, customer is awaiting a board. Was expected Friday or Today, didn't show. I asked if I could pay for expedited shipping, I seriously would have paid 100 bucks or more to get this thing next or second day'd, I gotta get this thing going. Oleg said theyd take care of the shipping, which i appreciate very much, i just dont know when its getting here. Called my LWS and have my finger on the trigger for a blue machine as I can't be down this week.

    And I need to add, I am very appreciative of Everlast sending me the part, instead of me sending my unit to them. I have been in contact with Oleg and Mark and know that they don't have the parts sitting in front of them to send to me, so there's more going on behind the scenes I'm sure. As with most break downs, it's extremely inopportune and is very close to forcing me to buy another machine just to do work. Not that I don't love the machine, I just have to keep on trucking.
    Last edited by WhitsonMetal; 07-20-2015 at 09:46 PM.

  16. Default

    Board is here! Going to take the solder gun to the shop and get this thing in asap.

  17. #17

    Default

    Quote Originally Posted by WhitsonMetal View Post
    Actually, customer is awaiting a board. Was expected Friday or Today, didn't show. I asked if I could pay for expedited shipping, I seriously would have paid 100 bucks or more to get this thing next or second day'd, I gotta get this thing going. Oleg said theyd take care of the shipping, which i appreciate very much, i just dont know when its getting here. Called my LWS and have my finger on the trigger for a blue machine as I can't be down this week.

    And I need to add, I am very appreciative of Everlast sending me the part, instead of me sending my unit to them. I have been in contact with Oleg and Mark and know that they don't have the parts sitting in front of them to send to me, so there's more going on behind the scenes I'm sure. As with most break downs, it's extremely inopportune and is very close to forcing me to buy another machine just to do work. Not that I don't love the machine, I just have to keep on trucking.
    WhitsonMetal

    jsut want to clear something .. we do stock parts and we do fix units. the part you need had to be programmed and we not yet set up for programming . programming unit should be set up in next month or so then we can do all programing locally and dont need to ask factory to do it
    Oleg Gladshteyn
    Phone: 650 588 8082 / 877 755 WELD
    Cell: 415 613 6664 ONLY IF YOU REALLY NEED IT
    Email: oleg@everlastwelders.com
    Website www.everlastgenerators.com

    www.linkedin.com/pub/oleg-gladshteyn/48/b08/875

  18. #18

    Default

    so what was wrong with the unit?
    250 ex
    205 mig
    milwaukee grinder
    140e mig

  19. Default

    Got the board in, fired up the machine and all seems well! Bummed that I lost all my memory settings but at least I can get back to work. I still don't see a thing wrong on the old board so I have no idea what exactly went wrong. I may look into having it rebuilt to keep on hand as a spare. Thanks very much for getting me the part, I was literally going to buy a machine today!

  20. #20

    Default

    Quote Originally Posted by WhitsonMetal View Post
    Got the board in, fired up the machine and all seems well! Bummed that I lost all my memory settings but at least I can get back to work. I still don't see a thing wrong on the old board so I have no idea what exactly went wrong. I may look into having it rebuilt to keep on hand as a spare. Thanks very much for getting me the part, I was literally going to buy a machine today!

    WhitsonMetal

    Board is actually fine, the software was corrupted somehow. All that board needed was to be flashed with new software
    Oleg Gladshteyn
    Phone: 650 588 8082 / 877 755 WELD
    Cell: 415 613 6664 ONLY IF YOU REALLY NEED IT
    Email: oleg@everlastwelders.com
    Website www.everlastgenerators.com

    www.linkedin.com/pub/oleg-gladshteyn/48/b08/875

Similar Threads

  1. Does Anyone Know? 325EXT
    By SteveY in forum TIG Welding (GTAW/GTAW-P)
    Replies: 3
    Last Post: 01-08-2019, 04:12 AM
  2. Mack Dump Truck and Lear Jet
    By cbmkr in forum On Road Fabrication
    Replies: 0
    Last Post: 07-28-2012, 10:17 PM
  3. Dump Trailer Repair
    By Jake98 in forum Welding Repairs
    Replies: 0
    Last Post: 01-22-2012, 04:10 PM
  4. Project #2 Cub Cadet dump truck
    By atatro in forum Hobyist Projects
    Replies: 4
    Last Post: 12-19-2011, 02:28 AM
  5. Project 3 from I_Love_Plasma ~ Parts/Firewood Dump Box
    By I_Love_Plasma in forum Heavy Equipment and Commercial Projects
    Replies: 0
    Last Post: 10-04-2011, 06:22 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •