    I just got in from my shop, I did a neat little mod that takes 20 minutes and will make your life a little easier. I added a quick connect to the gas inlet. I searched around and cannot find anything on the market, so I use what I find.

    First disconnect machine. Open'er up and disconnect the solenoid from the body, no need to unwire just treat it with respect. Remove the inlet fitting with two wrenches, one to support the solenoid, its in there tight. Cut the first couple barbs off and you should be left with about 3/8 of stem you can run a die over. I'm sure all of you have a 1/4 quick connect. Cut the threads off and drill to the appropriate size for mating tap, tapp'er out. Reassemble with teflon or dope, and replace sheet metal. All that is left is to put the female on the gas hose.

    If you are like me I go to different sites and I don't like to transport the machine with a regulator dangling off. Hope this helps.

  2. #2

    Default

    Thanks for the mod. Can you post a few photos? Also what size tap did you use?

  3. #3

    Default

    I have no digi cam so no pics yet. I also used a 8x1.125 tap and die.

Similar Threads

  1. Crossmemeber Modification Chevrolet Passenger Car
    By cbmkr in forum On Road Fabrication
    Replies: 9
    Last Post: 07-01-2014, 11:53 PM
  2. Custom 30 Ton Press Modification
    By cbmkr in forum Personal Projects (no welder required)
    Replies: 13
    Last Post: 09-27-2013, 08:30 PM
  3. VW front beam modification
    By youngnstudly in forum On Road Fabrication
    Replies: 0
    Last Post: 08-30-2013, 09:51 AM
  4. Project 3 from d3javoodoo # security modification #
    By Legacyartist247 in forum Hobyist Projects
    Replies: 0
    Last Post: 06-04-2011, 09:34 PM
  5. Honda Intake Manifold (TIG Weld) Modification
    By jakeru in forum On Road Fabrication
    Replies: 1
    Last Post: 03-07-2011, 05:18 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •