    Hello from Hazel Green, Alabama. I received my Super Ultra 205 yesterday and eagerly set it up. (I do not have any argon or tungsten so I was not able to use the TIG) I tried the stick welder and the Plasma Cutter. Since I have never used either of these I have no other reference to compare to. Even though I am currently hooked up to 110V I was able to make these work.

    I was a little disappointed in the 4 or 5 page broken English manual but was able to get by.

    I have a question. I thought I was purchasing a MOSFET machine but somewhere I saw a reference to an IGBT unit. I guess it does not matter to me... but just curious....

    Dennis
    Gasseous

    You will never win a horse race by yelling "Whoa!"

  2. #2
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Welcome to the forum. Be sure to download the online version of the manual. You will find it's much better than what's in the box.
    Long arc, short arc, heliarc and in-the-dark!

  3. #3

    Default

    http://www.everlastgenerators.com/si...tra%202014.pdf

    The online manual says mosfet. "IGBT Inverter Technology" is just part of the Everlast logo.
    I suggest 3/32 2% lanthanated tungsten to cover most of your tig welding and the largest argon bottle you can handle.
    I buy my tungsten from weldingcity.com http://www.weldingcity.com/tungsten-...thanated-blue/
    Welcome to the forum.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  4. #4
    Join Date
    Jul 2015
    Location
    Hazel Green, Alabama
    Posts
    18

    Default

    zoama,

    Thank you for the information. I am getting some 3/32 tungsten.... just have not ordered it yet.... I need to get the Argon but was thinking of the #2 bottle.... mainly because of price but also it is shorter... I am not a pro.... just a hobby welder... I started with the wire feed welder from HF.... decided to upgrade to do some sheet metal work on my 1965 VW.... now I have to learn how to TIG weld... LOL!!
    Gasseous

    You will never win a horse race by yelling "Whoa!"

  5. #5

    Default

    Quote Originally Posted by gasseous View Post
    zoama,

    Thank you for the information. I am getting some 3/32 tungsten.... just have not ordered it yet.... I need to get the Argon but was thinking of the #2 bottle.... mainly because of price but also it is shorter... I am not a pro.... just a hobby welder... I started with the wire feed welder from HF.... decided to upgrade to do some sheet metal work on my 1965 VW.... now I have to learn how to TIG weld... LOL!!
    I recommend going to your local steel supplier and buying a 21' stick of 2" flat 11 gauge (1/8") cold roll, 9 gauge (3/16") would be even better to practice. The cold roll steel doesn't have any mill scale to clean off before welding. Cut 4" pieces to practice running a bead with no filler. Once you've got that sorted move onto butting the edges of those pieces and practice butt welds with no filler. When you've got a handle on that start adding filler and work on other joint types. Watch all the tig welding videos on weldingtipsandtricks youtube channel https://www.youtube.com/user/welding...dtricks/videos Take your time and have fun.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

Similar Threads

  1. Everlast Green Fail
    By Rambozo in forum Customer Testimonials
    Replies: 1
    Last Post: 03-22-2018, 02:53 PM
  2. Going Green: 200DV
    By dumbwelder in forum TIG Welding (GTAW/GTAW-P)
    Replies: 36
    Last Post: 01-18-2017, 10:25 PM
  3. Hello from Green Bay
    By tcbetka in forum Introduce Yourself
    Replies: 7
    Last Post: 11-26-2012, 06:01 PM
  4. why buy green instead of red or blue?
    By backhoe in forum Introduce Yourself
    Replies: 29
    Last Post: 01-19-2012, 04:30 AM
  5. Any way to stop the green?
    By eide in forum Forum related Questions
    Replies: 13
    Last Post: 03-05-2011, 06:06 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •