  1. Default TIG Water cooler

    I just got a new w300 220v water cooler. Using it with a CK Flexloc 25' torch. I noticed when I look inside the the filler cap with the cooler running the return doesn't appear to have much pressure. It appears to be working but I just want be sure, and don't want to burn up a new torch. If anyone has one of these, could you let me know if this is normal.
    Thanks

  2. Default

    I don't have that cooler, but here's my experience with the one I have...

    It's a Miler and has a clear plastic tube where you can observe the coolant flow. I used it with that big, bulky, goofy torch that came with my PP256 and got used to seeing a pretty strong stream in it while running.

    I bought the 25' CK Flexloc and thought something was terribly wrong with it because that strong stream was barely a "trickle". I called CK because I too didn't want to burn-up my new torch. They told me it was normal to have just a trickle and, if I was really concerned, I could disconnect the return and run it into container. I forget the exact measurement that was the minimum, but I used a 24oz cup and it filled it in like 30 secs and that was over the amount I was told it should be by a fair amount...

  3. Default

    I thought the same thing. This cooler is suppose to run .26gpm. So I ran it into a 2 quart container in just under 2 minutes. So it seems to be right. It's good to hear CK says that's correct with the 25' torch. Makes me feel a little better.
    Thanks

Similar Threads

  1. W300 water cooler
    By bubbas55 in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 4
    Last Post: 12-05-2012, 01:53 AM
  2. Water cooler
    By srp in forum General Welding Questions
    Replies: 9
    Last Post: 07-10-2012, 08:05 AM
  3. Water cooler
    By hesstx in forum TIG Welding (GTAW/GTAW-P)
    Replies: 29
    Last Post: 11-12-2011, 09:19 PM
  4. DIY Water Cooler
    By acourtjester in forum Other Custom Fabrications
    Replies: 3
    Last Post: 06-10-2011, 03:22 AM
  5. water cooler fittings
    By johnson697 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 1
    Last Post: 06-02-2010, 01:12 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •