Share
Results 1 to 2 of 2

Thread: Pro 256 no HF (high frequency) start

  1. Default Pro 256 no HF (high frequency) start

    I get a good arc at the contact points when the machine first powers on, but no contact arcing or HF when I use the pedal.

    Just got off the phone with tech support, who had me turn the pre-flow down to zero, which did nothing to help. I was then issued a return authorization number.

    Is there anything else I should check or try before turning my welder over for 2+weeks and paying a buttload of shipping?

  2. #2
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by jch13 View Post
    I get a good arc at the contact points when the machine first powers on, but no contact arcing or HF when I use the pedal.

    Just got off the phone with tech support, who had me turn the pre-flow down to zero, which did nothing to help. I was then issued a return authorization number.

    Is there anything else I should check or try before turning my welder over for 2+weeks and paying a buttload of shipping?
    Check the switch in the pedal at the plug. Does the gas flow start as expected? Did you try the torch switch instead of the pedal? Does it weld normally with lift start?
    Long arc, short arc, heliarc and in-the-dark!

Similar Threads

  1. 250ex high frequency staying on
    By johnson697 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 5
    Last Post: 06-09-2014, 04:24 PM
  2. High Frequency Ground on back of 200DX
    By Shaggy in forum TIG Welding (GTAW/GTAW-P)
    Replies: 2
    Last Post: 02-23-2014, 09:57 AM
  3. New PP256, high frequency start not working
    By ScottRussell in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 17
    Last Post: 03-13-2013, 04:31 PM
  4. High-frequency ground and GFI breaker
    By MuttonHawg in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 9
    Last Post: 02-06-2013, 03:24 PM
  5. high frequency ground question
    By Wrenchtamer in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 1
    Last Post: 07-27-2010, 08:54 PM